Effects of spinning process and core yarn contents on yarn shape retention

机译:纺纱工艺和核心纱线含量对纱线形状保留的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Purpose In order to develop high shape retention yarn and investigate the effects of spinning process and core yarn contents on the shape retention of yarn, in this paper, three kinds of yarns, JC/T400 18.5tex (55.6dtex) core-spun yarn, JC/T400 18.5tex (44.4dtex) core-spun yarn and JC18.5tex pure cotton yarn were spun by using the complete condensing Siro-spinning technology. The paper aims to discuss these issues. Design/methodology/approach In this paper, the core-spun yarns were spun by using the complete condensing spinning and Siro-spinning technology. Two key spinning processes, yarn twist factor and core yarn pre-draft ratio, were optimized by using the orthogonal test method first. Then, via the variable control method, the position of the core yarn, the position of the bell mouth and the center distance between two bell mouths were optimized, respectively, and corresponding optimal spinning process of the three yarns was determined. Finally, the yarns were spun under the optimal process, and the performance of the spun yarns was tested and compared. Findings Results show that the yarn twist factor affects yarn strength and hairiness, the position of bell mouth affects the evenness and hairiness of the yarn mainly, and the position of the core yarn affects the coverage and hairiness of the yarn. For the Z-twist spinning, the core yarn enters the front roller from the left side of two strands center, which is beneficial to improve the covering effect of core yarn, and reduce the pilling phenomenon of the yarn. The contents of core yarn affect indicators of the yarn shape retention, such as yarn strength, elastic recovery and abrasion resistance. Originality/value The shape retention of yarns affects the shape retention of fabrics, and the production of yarn with high shape retention is a key step in achieving shape retention of fabrics. At present, there are little studies on the shape retention of yarns, most researchers shave focused on shape retention of fabrics. Using the complete condensing Siro-spinning method to spin the core-spun yarn can improve the quality of the yarn. Compared with traditional ring-spinning yarns, the addition of the core yarn can improve the shape retention of the yarn.
机译:目的是开发高形状保留纱,并研究纺纱工艺和核心纱线含量对纱线形状保留的影响,本文三种纱线,JC / T400 18.5TEX(55.6DTEX)核心纺纱纱, JC / T400 18.5TEX(44.4DTEX)核心纱线和JC18.5TEX纯棉纱线通过使用完全冷凝的Siro纺纱技术纺纱。本文旨在讨论这些问题。在本文中设计/方法/方法,通过使用完全的冷凝纺丝和Siro纺丝技术来旋转芯纺纱。通过首先使用正交试验方法优化两个关键纺丝工艺,纱线扭转因子和核心纱线比例。然后,通过可变控制方法,芯纱的位置,钟嘴的位置分别优化了两个钟嘴之间的中心距离,并且确定了三个纱线的相应最佳纺丝过程。最后,纱线在最佳过程下纺纱,测试并比较了纺纱纱的性能。研究结果表明,纱线扭曲因子影响纱线强度和毛羽,钟口的位置主要影响纱线的均匀性和毛羽,核心纱的位置影响纱线的覆盖和毛毛。对于Z-扭转纺丝,芯纱从两个股线中心的左侧进入前辊,这有利于提高核心纱的覆盖效果,并减少纱线的丸丸现象。核心纱线的含量影响纱线形状保留的指示器,例如纱线强度,弹性回收和耐磨性。原创性/值纱线的形状保持影响织物的形状保留,具有高形状保留的纱线的产生是实现织物形状保留的关键步骤。目前,对纱线的形状保留有很少的研究,大多数研究人员都剃须专注于形状保留织物。使用完全冷凝的Siro纺丝方法旋转芯纺纱可以提高纱线的质量。与传统的旋转纱线相比,加入芯纱可以改善纱线的形状保留。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号