This article presents the results of a study on the influence of adding 0.75% to 8% microcrystalline SS.B talc (from the Spanish talc producer Luzenac Set) to a porcellanato stoneware ceramic body. The soda feldspar and talc eutectic reduces the vitrification temperature in rapid firing cycles. It also improves the stain resistance of polished tiles. The study shows that the SiO_2/Al_2O_3 ratio should be constant and that the optimal content of SS.B talc is 3.2%. The bending resistance (MOR) is also improved by 20%. With its very low iron content, SS.B talc is particularly effective for the production of superwhite bodies containing zirconium because it does not affect the performance of the colouring agents in the body. The addition of SS.B talc has less effect on pyroplastic deformation than magnesite or wollastonite and is more efficient in improving stain resistance than dolomite and nepheline syenite.
机译:本文介绍了将0.75%至8%的微晶SS.B滑石粉(来自西班牙滑石粉生产商Luzenac Set)添加到porcellanato粗陶陶瓷体中的影响的研究结果。苏打长石和滑石共晶降低了快速烧结周期中的玻璃化温度。它还提高了抛光砖的耐污染性。研究表明,SiO_2 / Al_2O_3比值应保持恒定,SS.B滑石粉的最佳含量为3.2%。抗弯强度(MOR)也提高了20%。由于SS.B滑石粉中的铁含量非常低,因此它对生产含锆的超白体特别有效,因为它不影响体内着色剂的性能。与菱镁矿或硅灰石相比,添加SS.B滑石对热塑性变形的影响较小,并且与白云石和霞石正长岩相比,在提高抗污性方面更有效。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号