Effect of transverse field annealing and rate of cooling on magnetic properties of the amorphous Co/sub 71.5/Fe/sub 2.5/Mn/sub 2/Mo/sub 1/Si/sub 9/B/sub 14/ alloy

机译:横向场退火和冷却速率对非晶Co / sub 71.5 / Fe / sub 2.5 / Mn / sub 2 / Mo / sub 1 / Si / sub 9 / B / sub 14 /合金的磁性能的影响

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Influence of transverse field annealing (H/sub T/) and cooling rate (v/sub c/) on magnetic remanence (B/sub r/), coercivity (H/sub c/) and domain structure of the amorphous near-zero magnetostrictive Co/sub 71.5/Fe/sub 2.5/Mn/sub 2/Mo/sub 1/Si/sub 9/B/sub 14/ alloy was investigated. Two step magnetic annealing was performed on 20/spl times/15/spl times/10 mm toroidal cores and on 30/spl times/10 mm pieces of ribbons. Magnetic properties dependence upon a time of preannealing was determined too. Very strong effect of H/sub T/ and v/sub c/ on the magnetic properties and domain structure was discussed on the base of the Kronmuller model.
机译:横向场退火(H / sub T /)和冷却速率(v / sub c /)对非晶态接近零的剩磁(B / sub r /),矫顽力(H / sub c /)和畴结构的影响研究了磁致伸缩Co / sub 71.5 / Fe / sub 2.5 / Mn / sub 2 / Mo / sub 1 / Si / sub 9 / B / sub 14 /合金。在20 / spl次/ 15 / spl次/ 10mm环形磁芯和30 / spl次/ 10mm的薄带上进行两步磁性退火。还确定了取决于预退火时间的磁性能。在Kronmuller模型的基础上,讨论了H / sub T /和v / sub c /对磁性和畴结构的非常强的影响。