This paper presents a direct evaluation of the optimum lime content for treatment of expansive soils. Over fifty overburden swell tests were conducted in which samples treated with different percentages of hydrated lime were subjected to similar laboratory tests and the optimum lime content was determined. The test results indicated that the addition of lime is effective up to 2%, after which it starts to give a reverse effect on the swell characteristics of the tested soil. The swell percentage was twice that of the untreated soil for both 4% lime and 6% lime and about 1.75 that of the untreated soil for 8% lime. Curing time was found to reduce the amount of swell especially when the samples were treated with high percentage of lime. A new parameter termed the Lime Treatment Swell Ratio (LTSR) is introduced and used for characterizing the effectiveness of lime treatment Both volume change and swell pressure were found to be minimal for lime content of 1%. This is significantly lower than the 4% to 6% lime usually obtained based on the results of consistency indices, pH, and unconfined compressive strength tests.
机译:本文直接评估了处理膨胀土的最佳石灰含量。进行了五十多次上覆膨胀试验,其中对用不同百分比的熟石灰处理的样品进行了相似的实验室测试,并确定了最佳的石灰含量。试验结果表明,加入石灰有效至多2%,此后开始对试验土壤的膨胀特性产生相反的影响。对于4%石灰和6%石灰,膨胀百分比是未处理土壤的两倍,对于8%石灰,膨胀百分比是未经​​处理的土壤的约1.75。发现固化时间减少了溶胀量,特别是当样品用高百分比的石灰处理时。引入了一个新参数,称为石灰处理溶胀比(LTSR),用于表征石灰处理的有效性。对于石灰含量为1%的情况,体积变化和溶胀压力均最小。这明显低于根据稠度指数,pH和无限制抗压强度测试结果通常获得的4%至6%的石灰。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号