Physical and mechanical properties of concrete containing PET wastes as a partial replacement for fine aggregates

机译:宠物废弃物混凝土的物理和力学性能作为细骨料的部分替代品

获取原文
   

获取外文期刊封面封底 >>

       

摘要

In this study, the influence of using polyethylene terephthalate (PET) wastes as a partial replacement of natural sand is investigated to study the mechanical and physical properties of concrete. Fine aggregate (sand) is partially replaced by equivalent weight percentages of PET waste particles while maintaining all other proportions. Mechanical tests for compression, splitting, flexure, modulus of elasticity, energy absorption, and axial strain as well as physical tests for density, shrinkage, and absorption, are performed. In addition, the ultrasonic pulse velocity is presented. All specimens are observed for 7, 14, and 28 days. The tests results presented that the presence of PET particles changed the physical and mechanical properties of produced concretes. Physical properties (density and ultra sound velocity) gradually decreased as PET ratios increased, while an increase in absorption rate was observed. Furthermore, for strength-related properties, the results showed that the specimens containing partial substitution ratios ranging within 5 %–12.5 % displayed 26.8 %–43.64 %, 18.6 %–26.9 %, and 18.1 %–30.2 % increments in the compressive, tensile, and flexural strengths, respectively, compared with the reference specimens. The findings also revealed an increase in energy absorption and axial strain of the specimens with 5%–20 % replacement percentages, while the modulus of elasticity decreased as the PET content increased. The results further indicated that the strength parameters decrease when the PET content exceeds 15 %. In conclusion, replacing sand with waste PET particles positively affects the strength-related values of concrete specimens as long as the replacement ratio is less than 15 %.
机译:在该研究中,研究了使用聚对苯二甲酸乙二醇酯(PET)废物作为自然砂的部分替代的影响研究了混凝土的机械和物理性质。细骨料(沙子)部分地由PET废物颗粒的等效重量百分比替换,同时保持所有其他比例。进行机械测试,用于压缩,分裂,弯曲,弹性模量,能量吸收和轴向应变以及密度,收缩和吸收的物理测试。另外,提出了超声波脉冲速度。观察到所有标本7,14和28天。测试结果表明,PET颗粒的存在改变了产生的混凝土的物理和力学性能。随着PET比率的增加,物理性质(密度和超声速度)逐渐降低,而观察到吸收率的增加。此外,对于强度相关的性质,结果表明,含有部分取代比率范围内的试样为5%-12.5%显示26.8%-43.64%,18.6%-26.9%,压缩,拉伸的增量18.1%-30.2%。和与参考标本相比,分别弯曲强度分别。结果还揭示了试样的能量吸收和轴向菌株的增加,其替代百分比为5%-20%,而宠物含量增加,弹性模量降低。结果进一步表明,当PET含量超过15%时,强度参数降低。总之,只要替换率小于15%,替换废物宠物颗粒的砂砂就会积极地影响混凝土样本的强度相关值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号