首页> 外文期刊>SN Applied Sciences >The effect of randomly distributed natural fibers on some geotechnical characteristics of a lateritic soil
【24h】

The effect of randomly distributed natural fibers on some geotechnical characteristics of a lateritic soil

机译:随机分布的天然纤维对底层土壤岩土性特征的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Weak lateritic subgrades are more often than not encountered during road construction in Ghana. This makes it necessary to find economically efficient ways to improve the engineering properties of these marginal lateritic soils. The objective of this study is to investigate the effects of coconut fiber (30 mm, 60 mm and 90 mm fiber lengths) and palm fiber on some geotechnical characteristics of a weak lateritic subgrade. The lateritic soil was collected from the KNUST campus and blended with various percentages of the fibers varying between 0.1 and 1.0% by weight of dry soil. The mixed materials were then subjected to various laboratory tests including compaction, unconfined compression test and 4-day-soaked California bearing ratio test. From the results, it was observed that increasing the fiber content decreased the maximum dry density and increased the optimum moisture content. The inclusion of the fiber increased the soaked CBR from 7 to a maximum of 18, 22, and 25 at 30 mm, 60 mm and 90 mm fiber lengths, respectively. The unconfined compressive strength also increased from 140 to a maximum of 353 kPa, 398 kPa and 447 kPa, respectively, for 30 mm, 60 mm and 90 mm fiber lengths. Similarly, palm fiber inclusion recorded maximum soaked CBR value of 14% and UCS value of 352 kPa. These peak values were obtained at optimum fiber contents of 0.2%.
机译:在加纳的道路建设期间,薄弱的后面的路面比没有遇到。这使得有必要在经济上找到改善这些边际外形土壤的工程性质的经济有效方法。本研究的目的是探讨椰子纤维(30mm,60mm和90 mm纤维长度)和棕榈纤维对弱后退路基的一些岩土特征的影响。从剑兰校园中收集外晶土壤,并将各种百分比的纤维混合在0.1-1.0%(重量)的干燥土壤之间。然后对混合材料进行各种实验室试验,包括压实,非束缚的压缩试验和4天浸涂的加州轴承比试验。从结果中,观察到增加纤维含量的最大干密度降低并增加了最佳水分含量。将纤维的包含将浸泡的CBR增加至最大值为30mm,60mm和90mm纤维长度的7至最多18,22和25。非束缚的抗压强度分别从140升至最多353kPa,398kPa和447kPa,30mm,60mm和90mm纤维长度。类似地,棕榈纤维包涵体记录最大浸泡的CBR值14%,UCS值为352kPa。在最佳纤维含量为0.2%的最佳纤维含量下获得这些峰值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号