The aim of the present work was the obtaining and characterization of dental hybrid composites using nanoparticles (clay or silica) and boron-aluminum-silicate microparticles. We evaluated the dispersion of the nanofillers when changing their loading among 2.5%, 5%, 10% and 25% wt. Were tested, in the above quantities, four different types of nanofillers, two nanosilicas and two nanoclays The remainder of the inorganic phase, up to a total loading of 75% wt, was given by the boron-aluminum-silicate microparticles. The systems were characterized by XRD, TGA, LF-NMR, and . FTIR was used to determine the degree of conversion. The XRD and LF-NMR showed that the composites with 2.5% of clays, contained an exfoliated profile, and the groups with higher amounts of clay showed intercalated areas or the agglomeration of these particles. Furthermore, the silicas were agglomerated in all groups. The thermal resistance of the material was not affected by the silicas, but improved when using 2.5% of nanoclays. On the other hand, the addition of these particles caused the reduction of the degree of conversion of the systems.
机译:本作本作的目的是使用纳米颗粒(粘土或二氧化硅)和硼 - 硅酸铝微粒来获得和表征牙科杂化复合材料。当在2.5%,5%,10%和25%wt时,评估纳米填充物的分散。在上述量中测试了四种不同类型的纳米填料,两个纳米硅和两种纳米粘土的无机相的剩余部分,由硼 - 硅酸铝微粒给出了75%wt的总负荷。该系统的特征在于XRD,TGA,LF-NMR和。 FTIR用于确定转换程度。 XRD和LF-NMR显示,具有2.5%的粘土的复合材料含有剥落的曲线,并且具有较高量粘土的基团显示出插层的区域或这些颗粒的附聚。此外,二氧化硅在所有基团中凝聚。材料的热阻不受二氧化硅的影响,而是在使用2.5%的纳米粘土时改善。另一方面,添加这些颗粒导致减少系统的转换程度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号