Introduction. This in vitro study compared the shear strength of three composite resin systems to fluorosed and normal dentin. Methods. Silorane FiltekTM P90, FiltekTMZ250 XT in combination with the adhesive system AdperTM Single bond 2, and Amelogen? Plus in association with Peak Universal Bond? were tested. Fifteen normal and 15 fluorosed dentine disks were prepared per material. The shear bond strength test was performed using a universal machine. Results. One-way ANOVA revealed significant differences in bond strength between the tested composite resins. All tested materials had significantly different adhesion at the fluorosed and the nonfluorosed interface. FiltekTM Z250 XT and Silorane had lower adhesion values to fluorosed than to normal dentin. In contrast, Amelogen? Plus presented a better average resistance at the fluorosed interface. Conclusion. Amelogen? Plus presented a better average shear bond strength on the fluorosed dentine. FiltekTMZ250 XT showed the best adhesion forces and shear bond strength with sound dentine. Further studies are needed to better understand the sealing of these systems.
机译:介绍。这种体外研究将三种复合树脂体系的剪切强度与氟化和正常牙本质相比。方法。 Silorane Filtektm P90,Filtektmz250 XT与粘合剂系统Adpertm单键2,和Amelogen?另外与峰值通用债券有关吗?测试过。每种材料制备十五个正常和15个氟牙牙盘。使用通用机器进行剪切粘合强度试验。结果。单向ANOVA在测试的复合树脂之间揭示了粘合强度的显着差异。所有测试材料在氟化和非泡沫界面上具有显着不同的粘附性。 FILTEKTM Z250 XT和硅烷具有较低的粘附值,而不是正常的牙本质。相比之下,Amelogen?加上氟化界面的平均电阻更好。结论。 Amelogen?加上氟化牙本质上的平均平均剪切强度更好。 FILTEKTMZ250 XT显示出具有声音牙本质的最佳粘合力和剪切粘合强度。需要进一步研究以更好地理解这些系统的密封。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号