In this study, silver–strontium-doped hydroxyapatite (AgSr-HA)/chitosan composite coatings were deposited on a 316L stainless steel (SS) substrate via electrophoretic deposition (EPD). The Taguchi design of experiment (DoE) approach was used to optimize the EPD parameters such as the applied voltage, interelectrode spacing, and deposition time. Furthermore, the concentration of AgSr-HA particles in the suspension was also optimized via the DoE approach. DoE results demonstrated that the “homogeneous” coatings were obtained at the deposition time of 7 min, deposition voltage of 20 V, and at a concentration of 5 g/L AgSr-HA particles in the suspension. Scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), antibacterial studies, contact angle, and roughness measurements were performed to characterize the optimized coatings. SEM images confirmed the deposition of chitosan/AgSr-HA on the SS substrate. The wettability studies indicated the hydrophilic nature of the chitosan/AgSr-HA composite coatings, which confirmed that the developed coatings are suitable for biomedical applications, e.g., orthopedics. The average surface roughness of the chitosan/AgSr-HA composite coatings was in a suitable range used to attach the bone marrow stromal cells. Chitosan/AgSr-HA composite coatings showed an effective antibacterial effect against Gram-positive and Gram-negative bacteria. Moreover, the coatings developed apatite crystals on their surface upon immersion in simulated body fluid.
机译:在该研究中,通过电泳沉积(EPD)在316L不锈钢(SS)基板上沉积银锶掺杂的羟基磷灰石(AGSR-HA)/壳聚糖复合涂层。实验(DOE)方法的Taguchi设计用于优化EPD参数,例如施加的电压,电极间隔和沉积时间。此外,通过DOE方法优化悬浮液中AgSR-HA颗粒的浓度。 DOE结果证明,在7分钟的沉积时间,沉积电压为20V的沉积时间和悬浮液中以5g / L AgSR-HA颗粒的浓度获得“均相”涂层。扫描电子显微镜(SEM),能量分散X射线光谱(EDS),进行抗菌研究,接触角和粗糙度测量以表征优化的涂层。 SEM图像确认壳聚糖/ AGSR-HA沉积在SS衬底上。润湿性研究表明了壳聚糖/ AGSR-HA复合涂层的亲水性质,该涂层证实,发育涂层适用于生物医学应用,例如骨科。壳聚糖/ AGSR-HA复合涂层的平均表面粗糙度在适合于用于附着骨髓基质细胞的合适范围内。壳聚糖/ AGSR-HA复合涂料显示出针对革兰氏阳性和革兰氏阴性细菌的有效抗菌作用。此外,涂层在浸入模拟体液时在其表面上发育磷灰石晶体。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号