Two-body wear of occlusal splint materials against different antagonists

机译:针对不同拮抗剂的咬合夹板材料的两体磨损

获取原文

摘要

This study aimed to demonstrate that the material of the occlusal splint can be chosen according to the needs of individual patients and contribute to the knowledge of the wear rate of these materials. In this study, four occlusal splint materials (Sr Ivocap Heat Cured, Valplast, SR Ivocap Elastomer and Eclipse) and three antagonists (natural tooth enamel, inCoris TZI and IPS e.max Press ceramic materials) were used. Each wear test was performed using a chewing simulator (n?=?16; test load: 50?N; number of cycles: 10,000, 20,000 and 30,000; continuous rinsing with water at 30?°C for the wet condition). The Shapiro Wilk test was used for normal distribution suitability. Antagonist on average wear quantities both main effects and interactions of material, cycle and condition factors were investigated by Univariate variance analysis. Multiple comparisons were examined using the Games-Howell test. There was a statistically significant effect of the difference in materials on the amount of wear (p 0.001). The highest mean value was obtained with Eclipse (0,318?μm3), and the lowest mean value was obtained with Valplast (0,134?μm3). Our study found differences in the in vitro wear rate among various occlusal splint materials.
机译:本研究旨在证明可以根据个体患者的需求选择咬合夹板的材料,并有助于这些材料的磨损率的知识。在本研究中,使用四种咬合夹板材料(SR IVocap热固化,valplast,SR IVocap弹性体和Eclipse)和三个拮抗剂(天然牙齿搪瓷,菊苣TZI和IPS E.max Bress陶瓷材料)。使用咀嚼模拟器进行每个磨损试验(n?=Δ16;测试载荷:50?n;循环次数:10,000,20,000和30,000;连续用水冲洗30.°C的潮湿条件)。 Shapiro Wilk测试用于正常分配适用性。通过单变量方差分析研究了平均磨损量的平均磨损量的主要效果和相互作用。使用Games-Howell测试检查多种比较。材料差异对磨损量的差异有统计学显着的影响(p 0.001)。用Eclipse(0.318Ωμm3)获得最高平均值,并用甘蔗(0,134Ωμm3)获得最低平均值。我们的研究发现了各种咬合夹板材料中的体外磨损率的差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号