Comparative Evaluation of Tensile ? Bond Strength of An Orthodontic Adhesive with and without Fluoride Application, After Acid Etching -An Invitro Study

机译:拉伸强度的比较评价酸蚀后使用和不使用氟化物的正畸胶粘剂的结合强度-体外研究

获取原文
           

摘要

Background: Fixed appliances hinder the effective control of plaque accumulation and white spot lesions may develop under the ill fitting bands or adjacent to the stainless steel brackets during orthodontic treatment particularly the etching process. Aims and Objectives: Comparative study of tensile bond strength of an orthodontic adhesive with and without fluoride application after acid etching to know the effect of fluoride on bond strength. Materials and Methods: This study is carried out on 90 non carious human premolar teeth, and divided in 6 groups with each group of 15 specimens. In those Groups I and IV were control group acid etch treatment, Group II and V is 1.23% APF gel (acid etch plus APF gel treatment,) and group III and VI is 8% SnF2 (acid etch plus SnF2 treatment). Samples of Group I, II and III bond strength were tested after 24 h and groups IV, V and VI after one month on microtechtensometer machine. The scanning electron microscope (SEM) investigation was carried out for the 2 specimens for the control group after acid etch and 4 specimens after acid etch with fluoride application for fluoride groups. Results: Control and SnF2 treated groups was found to be nearly similar to the control group whereas APF treated group showed less focal holes than the other 2 groups. Conclusion: Fluoride application after acid etching without having an adverse effect on bond strength but we can prevent the white spot lesions and caries.
机译:背景:固定的矫形器妨碍了对斑块积聚的有效控制,在正畸治疗(尤其是蚀刻工艺)期间,在不适的固定带下或不锈钢支架附近可能会形成白斑病变。目的和目的:对比研究酸蚀后使用和不使用氟化物的正畸粘合剂的拉伸粘结强度,以了解氟化物对粘结强度的影响。材料和方法:本研究是对90颗人类非龋性前磨牙进行的,分为6组,每组15个样本。在那些I和IV组中,对照组进行酸蚀刻处理,II和V组为1.23%APF凝胶(酸蚀刻加APF凝胶处理),III和VI组为8%SnF2(酸蚀刻加SnF2处理)。 I,II和III组的结合强度样品在24小时后测试,IV,V和VI组在一个月后用微技术强度仪测试。对酸蚀后的对照组的2个样本和酸蚀后的4个样本进行了扫描电子显微镜(SEM)研究,其中氟化物施加了氟。结果:发现对照组和SnF2处理组与对照组几乎相似,而APF处理组的焦孔比其他两组少。结论:酸蚀后施加氟化物不会对粘结强度产生不利影响,但可以预防白斑病变和龋齿。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号