A novel MgSrLa8?x(SiO4)6O2:xEu (MSLSO:xEu) phosphor was synthesized through a high-temperature solid-state reaction. The crystal structures, luminescent properties, fluorescence decay time, and oxygen vacancies were investigated systemically. XRD analysis shows a typical oxyapatite structure with the space group P63/m. Europium can enter crystal matrices simultaneously in the form of Eu3+ and Eu2+ and occupy nonequivalent crystallographic positions in a lattice, thus forming various optical centers. Under ultraviolet light excitation, the phosphors simultaneously show the blue-green emission of Eu2+ and the green-yellow-red emission of Eu3+. The optimal doping content of Eu is 7.5 mol% (x = 0.075). White light can be realized with a CIE coordinate of (0.3664, 0.3260) by adjusting the concentration of Eu. The lifetimes of Eu3+ and Eu2+ in this study are considerably longer than those in other references. The results suggest that the MSLSO:Eu2+/Eu3+ (0.075) phosphor is a promising candidate for white LEDs.
机译:一种新颖的MgSrLa 8? x (SiO 4 6 O 2 x Eu(MSLSO: x Eu)荧光粉通过高温固态反应合成。系统地研究了晶体结构,发光性能,荧光衰减时间和氧空位。 XRD分析显示了典型的羟磷灰石结构,其空间群为 P 6 3 / m 。 can可以以Eu 3 + 和Eu 2 + 的形式同时进入晶体基质,并占据非等价晶体位置在一个格子中,从而形成各种光学中心。在紫外光激发下,磷光体同时显示Eu 2 + 的蓝绿色发射和Eu 3+的绿黄色红色发射。 。 Eu的最佳掺杂含量为7.5mol%( x = 0.075)。通过调节Eu的浓度,可以用CIE坐标(0.3664,0.3260)实现白光。本研究中Eu 3 + 和Eu 2 + 的寿命比其他参考文献中的寿命长。结果表明,MSLSO:Eu 2 + / Eu 3 + (0.075)荧光粉是有前途的候选材料用于白色LED。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号