This paper reports the results from laboratory studies on the compressive strength of mortar for Ferro cement that contains ternary blends of Portland cement, silica fume and super plasticizer as water reducing agent. Cement mortars (1:2, 1: 2.5 and 1:3) incorporating various water cementitious ratios (0.32, 0.35 and0.38) were used. The silica fume content is constant at 5% by weight of cement. Fly ash content varying from 10% to 20% and super plasticizer were used to maintain uniform flow of mortar which varies from 0% to 1% by weight of cement, to ensure that no segregation would occur. Totally 586 mortar cubes for each mix with mineral admixtures were tested for their compressive strength. Finally suggestions were made for the proportion of mineral admixtures to achieve high strength mortar which can be used for rehabilitation of reinforced concrete structures particularly with Ferro cement composites.
机译:本文报告了有关砂浆对Ferro水泥的抗压强度的实验室研究结果,该砂浆包含波特兰水泥,硅粉和高效减水剂的三元共混物作为减水剂。使用结合了各种水胶凝比(0.32、0.35和0.38)的水泥砂浆(1:2、1:2.5和1:3)。硅粉含量恒定为水泥重量的5%。粉煤灰含量从10%到20%不等,使用超级增塑剂来保持砂浆的均匀流动(水泥重量从0%到1%不等),以确保不会发生偏析。对于每种掺有矿物掺合料的混合物,共测试了586砂浆立方体的抗压强度。最后提出了关于矿物掺合料的比例的建议,以实现高强度砂浆,该砂浆可用于钢筋混凝土结构的修复,特别是与Ferro水泥复合材料的修复。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号