Research on Degumming and Fixing Sericin to Obtain Sericin-fixed Souple Silk Yarns without Formaldehyde

机译:脱胶固定丝胶获得无甲醛丝胶固定双丝的研究

获取原文
   

获取外文期刊封面封底 >>

       

摘要

In order to obtain sericin-fixed souple silk yarns, various conditions of degumming and fixing sericin were investigated. When raw silk yarns were degummed with solutions of soap and sodium carbonate and then fixed with sericin-fixing agents, degumming losses of 6-17% were attained. The degumming losses attained by degumming and fixing simultaneously in a solution of soap and sodium carbonate containing sericin-fixing agents were in the range of 6-9 percent. By one-step degumming with detergent after fixing sericin, sericin-fixed souple silk yarns were also obtained. In the case of two-step degumming successively twice at 60°C for 30 minutes and at 80°C for 30 minutes with detergent after fixing sericin at 60-80°C for 15 minutes with melamine and formaldehyde, the degumming losses were in the range of 7-13% and sericin removal was uniform. Two-step degumming was very effective for the elimination of free formaldehyde from silk yarns fixed with melamine and formaldehyde.
机译:为了获得丝胶蛋白固定的汤匙丝纱线,研究了各种条件对丝胶蛋白进行脱胶和固定。将生丝用肥皂和碳酸钠溶液脱胶,然后用丝胶固定剂固定后,脱胶损失为6-17%。通过同时在含有丝胶固定剂的肥皂和碳酸钠溶液中进行脱胶和固定而获得的脱胶损失在6-9%的范围内。固定丝胶后,通过用洗涤剂进行一步脱胶,也获得了丝胶固定的汤丝丝。在用三聚氰胺和甲醛将丝胶在60-80°C下固定15分钟后,在60°C下连续30分钟,在80°C下连续30分钟用去污剂两次脱胶的情况下,脱胶损失在范围为7-13%,丝胶去除率是均匀的。两步脱胶对消除三聚氰胺和甲醛固定的丝纱线中的游离甲醛非常有效。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号