Wetspun nascent PAN fibers were immersed into a DMSO/H2O coagulation bath. Diffusion of DMSO from nascent fiber and that of H2O into nascent fiber were studied at different temperatures and concentrations of coagulation bath. The diffusion coefficient of H2O is larger than that of DMSO. As the coagulation bath temperature increased, the diffusion coefficients of DMSO and H2O increased. Diffusion activation energy of DMSO is smaller than that of H2O during the diffusion. Cross sectional and surface structure of nascent PAN fiber were observed in relation to coagulation ability (the product of diffusion coefficients of two solvents). Coagulation ability was found to have a significant influence on both the cross sectional and surface morphology of nascent fiber. To obtain nascent fiber with circular cross sectional and smooth surface morphology, coagulation ability should be controlled at low value
机译:将湿纺新生PAN纤维浸入DMSO / H2O凝固浴中。研究了在不同温度和凝结浴浓度下,DMSO从新生纤维中的扩散以及H2O在新生纤维中的扩散。 H2O的扩散系数大于DMSO。随着凝结浴温度的升高,DMSO和H2O的扩散系数增加。在扩散过程中,DMSO的扩散活化能小于H2O。观察到新生PAN纤维的横截面和表面结构与凝结能力(两种溶剂的扩散系数的乘积)有关。发现凝结能力对新生纤维的横截面和表面形态均具有显着影响。为了获得具有圆形横截面和光滑表面形态的新生纤维,应将凝结能力控制在较低值

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号