In?vitro compressive fracture resistance of?human maxillary first premolar with different mesial occlusal distal cavity

机译:不同上颌咬合远端腔的人上颌第一前磨牙的体外抗压性骨折

获取原文
           

摘要

Background/purposeThe purpose of this study was to determine fracture loads of human maxillary first premolars restored with condensable composite resin (Surefil, Dentsply) or leucite-reinforced ceramic inlays (ProCAD, Ivoclar Vivadent) in mesial occlusal distal cavity preparations of differing pulpal depths and isthmus widths.Materials and methodsNinety freshly extracted intact maxillary first premolars were divided into nine groups of 10. One group was an unprepared control. Eight groups of teeth were prepared to create different widths and depths of mesial occlusal distal cavities. Subsequently, teeth were restored with either condensable composite resin or ceramic inlay. Specimens were then subjected to axial loading with a 4.82-mm diameter steel ball in a universal testing machine at a crosshead speed of 0.5?mm/minute. Loads were applied against tooth structure, and the steel ball did not contact restorative material. Data were analyzed with multiple analysis of variance and Tukeypost hoctesting.ResultsMean fracture load of teeth restored with Surefil and a 3-mm cavity width was greater than in groups with a 2-mm cavity width (P?=?0.0315). Teeth restored with ProCAD were observed to have significantly higher mean cusp fracture load compared to teeth restored with composite resin (P?=?0.0003).ConclusionA bonded ceramic restoration restores the fracture load of a tooth comparable to an intact tooth independent of the examined design parameters, whereas the fracture loads of composite-resin-restored teeth were dependent on cavity widths. Cavity pulpal floor depth is not a significant factor of cusp fracture resistance in a tooth restored with either a ceramic inlay or composite resin.
机译:背景/目的这项研究的目的是确定在不同牙髓深度和不同牙髓的近中颌咬合远端腔准备中使用可凝结的复合树脂(Surefil,Dentsply)或白云石增强的陶瓷嵌体(ProCAD,Ivoclar Vivadent)修复的人类上颌第一前磨牙的骨折负荷。材料和方法将90个新鲜提取的完整的上颌第一前磨牙分为9组,每组10个。一组是未准备好的对照。准备八组牙齿以产生不同的宽度和深度的近中咬合远端腔。随后,用可凝结的复合树脂或陶瓷嵌体修复牙齿。然后在万能试验机中用直径为4.82毫米的钢球以0.5毫米/分钟的十字头速度对试样进行轴向载荷。对牙齿结构施加了载荷,并且钢球没有接触修复材料。结果通过Surefil和3 mm腔宽修复的牙齿平均骨折负荷大于2 mm腔宽的组(P?=?0.0315)。观察到用ProCAD修复的牙齿与使用复合树脂修复的牙齿相比具有更高的平均尖牙断裂负荷(P?=?0.0003)。结论结合陶瓷修复体可以使牙齿的断裂负荷与完整的牙齿相当,而与所检查的设计无关参数,而复合树脂修复牙齿的断裂载荷则取决于型腔宽度。在用陶瓷嵌体或复合树脂修复的牙齿中,牙髓根底深度不是抗尖锐断裂性的重要因素。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号