Activated-Carbon-Supported Phosphotungstic Acid as Novel Heterogeneous Catalysts for Cationic Polymerization of β-Pinene

机译:活性炭负载的磷钨酸是β-ogen烯阳离子聚合的新型多相催化剂

获取原文
           

摘要

References(23) Cited-By(1) Activated-carbon-supported phosphotungstic acid (HPW/C) catalysts were prepared and characterized by FT-IR spectroscopy, X-ray diffraction (XRD), scanning electron microscopy (SEM), and the Brunauer–Emmett–Teller (BET) method. The catalytic performance of HPW/C for β-pinene polymerization was also investigated. The characterization results show that the Keggin structure of HPW does not change after being supported on the activated carbon. The tiny particles of HPW are distributed amorphously and uniformly on the surface of the activated carbon. HPW can interact strongly with surface oxygen-containing groups on the activated carbon. The immobilization of HPW leads to a decrease in the specific surface area and total porous volume of the activated carbon. The polymerization conditions were optimized as follows: loading amount 34.2 wt%; dosage of catalysts 0.6 g; reaction temperature 0–10°C; β-pinene 3 mL; solvent 7 mL; reaction time 2 h. Under these conditions, the polymer yield was up to 73.0%, and the number-average molecular weight was about 860.
机译:参考文献(23)引用了(1)活性炭负载的磷钨酸(HPW / C)催化剂,并通过FT-IR光谱,X射线衍射(XRD),扫描电子显微镜(SEM)和Brunauer–Emmett–Teller(BET)方法。还研究了HPW / C对β-pine烯聚合的催化性能。表征结果表明,HPW的Keggin结构在负载在活性炭上后不会改变。 HPW的细小颗粒无定形且均匀地分布在活性炭的表面上。 HPW可以与活性炭上的表面含氧基团强烈相互作用。 HPW的固定导致活性炭的比表面积和总孔体积的减少。聚合条件的优化如下:负载量34.2 wt%;催化剂用量0.6μg;反应温度0-10℃; β-pine烯3 mL;溶剂7 mL;反应时间2 h。在这些条件下,聚合物的产率高达73.0%,并且数均分子量为约860。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号