This work describes a hydrometallurgical route for processing spent commercial catalysts (CoMo and NiMo/Al2O3). Samples were preoxidized (500 oC, 5 h) in order to eliminate coke and other volatile species present. The calcined solid was dissolved in concentrated H2SO4 and water (1:1 vol/vol) at 90 oC; the insoluble matter was separated from the solution. Molybdenum was recovered by solvent extraction using tertiary amines at pH around 1.8. Cobalt (or nickel) was separated by addition of aqueous ammonium oxalate at the above pH. Phosphorus was removed by passing the liquid through a strong anion exchange column. Aluminum was recovered by neutralizing the solution with NaOH. The route presented in this work generates less final aqueous wastes because it is not necessary to use alkaline medium during the metal recovery steps.
机译:这项工作描述了湿法冶金路线,用于处理用过的商用催化剂(CoMo和NiMo / Al2O3)。将样品预氧化(500 oC,5 h)以消除焦炭和其他存在的挥发性物质。将煅烧的固体在90 oC溶于浓H2SO4和水(1:1 vol / vol);从溶液中分离出不溶物。通过在pH约为1.8的条件下使用叔胺通过溶剂萃取来回收钼。通过在上述pH下加入草酸铵水溶液分离钴(或镍)。使液体通过强阴离子交换柱除去磷。通过用NaOH中和溶液来回收铝。由于不需要在金属回收步骤中使用碱性介质,因此在这项工作中提出的路线产生的最终含水废物较少。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号