This work describes a process for metal recovery from spent NiMo and CoMo/Al2O3 commercial hydrorefining catalysts. The samples were treated by fusion with potassium hydrogen sulfate (5 h, 600 ?oC) with a KHSO4/catalyst mass ratio of 10:1. After fusion the solid was solubilized in water (100 ?oC), leaving silicon compounds as residue. Losses of nickel and cobalt may reach 16 wt% of the amount present in the sample, depending on the silicon content. Soluble metals were isolated by selective precipitation techniques (nickel, cobalt, aluminum) or by solvent extraction with methyl-isobutyl ketone (molybdenum) in a hydrochloric acid medium. All metals were recovered in very good yields except for nickel and cobalt in the presence of considerable amounts of silicon. Soluble wastes consist of potassium/sodium sulfates/chlorides. Solid wastes correspond to about 4 wt% of the catalyst and can be discarded in industrial dumps.
机译:这项工作描述了从废NiMo和CoMo / Al2O3商业加氢精制催化剂中回收金属的方法。用KHSO4 /催化剂质量比为10:1的硫酸氢钾(5 h,600°C)熔融处理样品。熔融后,将固体溶于水(100°C),剩下硅化合物作为残留物。根据硅含量的不同,镍和钴的损失可能达到样品中镍和钴含量的16%(重量)。通过选择性沉淀技术(镍,钴,铝)或通过在盐酸介质中用甲基-异丁基酮(钼)进行溶剂萃取来分离可溶性金属。除存在大量硅的情况下的镍和钴外,所有金属的回收率都很高。可溶性废物包括钾/硫酸钠/氯化物。固体废物约占催化剂的4 wt%,可在工业垃圾场中丢弃。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号