This work presents a study on the dissolution of some commercial monometallic and non-supported deactivated catalysts in HF + H2O2 mixtures (and, eventually, other media) under mild experimental conditions, after a previous oxidation step. The samples were neither crushed nor grinded. The best experimental conditions were dependent on the nature of the support and of the active phase. For example, the Pt/Al2O3 catalyst was dissolved in about 10 minutes, without agitation and heating; however, dissolution of the Pd/Al2O3, Ni/Al2O3, Ni/SiO2, Cu/Al2O3 and V2O5 samples required a temperature of 60 oC and an agitation of 400 rpm. A careful addition of a NaOH solution allowed a quantitative precipitation of aluminium as criolite (Na3AlF6) or precipitation of Si as Na2SiF6; NaF was obtained as a by-product. As expected, processing of Pd/C, V2O5 and CuO.Cr2O3 samples was relatively simple. Metals recovery from catalysts reached a quantitative level in all samples studied; it is particularly interesting that platinum and palladium could be easily recovered in a single step process, thus separing them from aluminium.
机译:在先前的氧化步骤之后,这项工作提出了在温和的实验条件下,将某些市售单金属和非负载失活催化剂在HF + H2O2混合物(以及最终其他介质)中的溶解性研究。样品既不粉碎也不粉碎。最佳实验条件取决于载体和活性相的性质。例如,Pt / Al2O3催化剂在不搅拌和加热的情况下在约10分钟内溶解。但是,Pd / Al2O3,Ni / Al2O3,Ni / SiO2,Cu / Al2O3和V2O5样品的溶解需要60 oC的温度和400 rpm的搅拌。小心地添加NaOH溶液,可以定量沉淀出铝为堇青石(Na3AlF6)或Si为Na2SiF6。获得NaF作为副产物。不出所料,Pd / C,V2O5和CuO.Cr2O3样品的处理相对简单。在所有研究的样品中,从催化剂中回收的金属均达到定量水平。特别有趣的是,铂和钯可以在一个步骤中轻松回收,从而将它们与铝分离。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号