One of the disadvantages of shear thickening fluid (STF) is high concentration. For better immersion of fibers, at first STF is diluted in ethanol, and then the fibers are left therein for a specified period in order to impregnate all fibers with the fluid. After this stage, to eliminate the ethanol in the sample, it is heated at a temperature range of 60–80°C. The composite’s sensitivity to the impact will be reduced through ethanol combining with the fluid and its elimination. Furthermore, by means of vacuum infusion processing method, without use of ethanol (or reducing its portion) and heating, lighter composite could be obtained. The fluid is distributed to the required extent among the fibers and the additional fluid that causes weight increase is discharged through vacuum. In addition, the bubbles among the fibers and fluid are removed by vacuum. Specimens with 3 and 5 layers have been tested. By comparing the nanocomposites and neat specimens, experimental results show higher ballistic limit in all of the nanocomposite specimens. Results show that the ballistic limit is highest in the VIP method.
机译:剪切增稠流体(STF)的缺点之一是高浓度。为了更好地浸入纤维,首先将STF稀释在乙醇中,然后将纤维在其中保留指定的时间,以便用流体浸渍所有纤维。此阶段之后,为了消除样品中的乙醇,将其在60-80°C的温度范围内加热。通过将乙醇与液体结合并消除,可降低复合材料对撞击的敏感性。此外,借助于真空灌注处理方法,无需使用乙醇(或减少乙醇的比例)和加热,就可以获得较轻的复合材料。流体以所需的程度分布在纤维之间,导致重量增加的其他流体通过真空排出。另外,通过真空除去纤维和流体之间的气泡。具有3层和5层的样品已经过测试。通过比较纳米复合材料和纯净的标本,实验结果表明,所有纳米复合材料标本的弹道极限都更高。结果表明,VIP方法的弹道极限最高。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号