The present study addresses the direct flotation route for the concentration of a zinc silicate ore. Flotation of hemimorphite faces some challenges due to the similarity of hemimorphite and quartz surface properties. XRD, and XRF analyses, optical mineralogy and SEM with X-ray mapping were performed for characterization. The results showed that the quartz, hemimorphite, calcite and dolomite are the main minerals. In the flotation process, combined form of Octadecylamine and Armac T, as mixed cationic collectors were introduced. Flotation tests were employed in two steps to evaluate the individual effect of the variables such as: size distribution of feed and the presence of Armac T in the first step, alkalinity, types and concentrations of reagents (Armac T and stearyl amine (collectors), sodium sulfide (sulphidizing agent), and sodium hexametaphosphate (dispersant) in the second step. In optimal conditions, the grade and recovery of zinc in concentrate were ~33 % and 83 %, respectively. Finally, for removing the detrimental effect of fine particles, de-sliming of pulp feed accomplished which resulted in a remarkable increase in the recovery of hemimorphite concentrate (12.67%) and a decrease in the grade of zinc in tailing (6.11%). FTIR analysis showed the adherence of collectors on hemimorphite particles increased after de-sliming.
机译:本研究解决了硅酸锌矿石浓缩的直接浮选路线。由于半晶石和石英表面性质的相似性,使半晶石的浮选面临一些挑战。进行了XRD和XRF分析,光学矿物学和具有X射线映射的SEM进行表征。结果表明,石英,半晶石,方解石和白云石是主要矿物。在浮选过程中,引入了十八烷基胺和Armac T的混合形式,作为混合的阳离子捕收剂。浮选试验分两个步骤进行,以评估变量的单独影响,例如:饲料的粒度分布和第一步中Armac T的存在,碱度,试剂的类型和浓度(Armac T和硬脂胺(收集器),第二步是硫化钠(硫化剂)和六偏磷酸钠(分散剂),在最佳条件下,精矿中锌的品位和回收率分别为〜33%和83%,最后消除了细颗粒的有害影响,完成了纸浆进料的去粘,从而使半晶石精矿的回收率显着提高(12.67%),尾矿中锌的品位降低(6.11%)。FTIR分析表明,捕收剂对半晶石颗粒的附着力增加了除泥后。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号