The article discusses the impact of surface preparation method of Inconel 625 and 718 nickel-base alloys in the form of sheets on wettability of the surface. The results of the investigations of surface preparation method (such as nicro-blasting, nickel plating, etching, degreasing, abrasive blasting with grit 120 and 220 and manually grinding with grit 120 and 240) on spreading of BNi-2 and BNi-3 brazing filler metals, widely used in the aerospace industry in high temperature vacuum brazing processes, are presented. Technological parameters of vacuum brazing process are shown. The macro- and microscopic analysis have shown that nicro-blasting does not bring any benefits of wettability of the alloys investigated.
机译:本文讨论了片状Inconel 625和718镍基合金的表面制备方法对表面润湿性的影响。对BNi-2和BNi-3钎焊扩散的表面处理方法(如喷砂,镀镍,蚀刻,脱脂,用砂砾120和220进行喷砂以及用砂砾120和240进行手动研磨)的研究结果。介绍了在高温真空钎焊工艺中广泛用于航空航天工业的填充金属。显示了真空钎焊工艺的技术参数。宏观和微观分析表明,喷砂处理并没有带来所研究合金润湿性的任何好处。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号