This study evaluated the effect of aging methods on the bond strength of etch-and-rinse adhesive systems to dentin cavities. Eighty bovine incisors were used to prepare dentin cavities, which were bonded with different adhesive systems [Adper Scotchbond Multipurpose (SBMP), and Adper Single Bond 2 (SB)], and restored with composite resin. The specimens were stored in water for 24?h, and subjected to each aging method (n?=?10): control group (not exposed to additional aging), thermal cycling (TC) (10,000 cycles; at temperatures of 5, 37, and 55?°C), mechanical loading (ML) (100,000 cycles; Hz; 60?N load), and TC?+?ML. The push-out bond strength test was performed using a universal testing machine. Failure modes were evaluated by scanning electron microscopy. Data were analyzed by two-way ANOVA and Tukey’s test (α?=?0.05). For SBMP, only TC?+?ML decreased the bond strength compared to control group. For SB, all aging methods decreased similarly the bond strength compared to control group. A high number of adhesive failures were observed. Therefore, SB was sensitive to all aging methods, whilst only TC?+?ML was able to decrease the bond strength for SBMP.
机译:这项研究评估了老化方法对蚀刻和漂洗粘合剂系统与牙本质腔的粘合强度的影响。用八十个牛切牙准备牙本质腔,用不同的粘合剂系统粘合[Adper Scotchbond Multipurpose(SBMP)和Adper Single Bond 2(SB)],并用复合树脂修复。将样品在水中保存24小时,并采用每种老化方法(n≥10):对照组(不进行额外老化),热循环(TC)(10,000个循环;温度为5、37) ,以及55?C),机械负载(ML)(100,000个周期; Hz; 60?N负载)和TC?+?ML。使用通用测试机进行推出粘合强度测试。通过扫描电子显微镜评估失效模式。数据通过双向方差分析和Tukey检验(α?=?0.05)进行分析。对于SBMP,与对照组相比,只有TCα+βML降低了结合强度。对于SB,与对照组相比,所有老化方法均会类似地降低粘结强度。观察到大量的粘合失败。因此,SB对所有老化方法都敏感,而只有TCα+ΔML能够降低SBMP的结合强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号