Effect of Long-time Heating for Polyvinyl Chloride and Polypropylene Resin Pellet Certified Reference Materials for Heavy Metal Analysis

机译:长期加热聚氯乙烯和聚丙烯树脂颗粒认证的重金属分析参考材料的影响

获取原文
           

摘要

The effect of long-time heating for both polyvinyl chloride (PVC) and polypropylene (PP) resin pellet certified reference materials (CRMs) for heavy metal analysis, which contained Cd, Cr, Hg and Pb, was examined in the present study. The temperature of the drying oven was 80°C, which was used for drying these CRMs before analysis, and the long-time heating was carried out for up to 480 h. As a result, a relative decrease in mass of ca. 0.3% was observed for both CRMs. Moreover, a decrease in concentration of ca. 10% was observed for Cr, even though the concentrations for other elements did not change during the long-time heating. Since the chemical form of Cr was an organometallic compound with lower melting point, it was considered that concentration decreased due to the heat.
机译:在本研究中,研究了长期加热聚氯乙烯(PVC)和聚丙烯(PP)树脂颗粒认证的重金属分析参考材料(CRM)的影响,这些参考材料包含Cd,Cr,Hg和Pb。干燥箱的温度为80°C,用于在分析前干燥这些CRM,并进行了长达480小时的长时间加热。结果,ca的质量相对降低。两种CRM的观察结果均为0.3%。此外,浓度降低。即使在长时间加热期间其他元素的浓度没有变化,也观察到Cr为10%。由于Cr的化学形式是具有较低熔点的有机金属化合物,因此认为其浓度由于热而降低。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号