With a modified instrument for the testing bitumen hardness the authors have tested the hardness of the commercial pink wax in a number of temperature intervals ranging from 10CC to 30°C. This range, especially that about 20°C, is important in the prosthetic clinical proctice when the impression wax is used in combination with the elastomeres. It was found that this range is the most critical and that the pink wax produced in our country is most quickly-hardened when cooled between 19°C and 22°C. Therefore this range must be avoided by means of undercooling. Addition of the stearine acid 0,25% — 0,50% to the pink wax significantly improves its hardness properties.
机译:作者使用改进的测试沥青硬度的仪器,在从10CC到30°C的多个温度范围内测试了商用粉蜡的硬度。当压印蜡与弹性体组合使用时,该范围,尤其是约20°C的范围对于假肢临床操作非常重要。发现该范围是最关键的,并且在我国冷却的温度在19°C至22°C之间时,生产的粉红色蜡固化最快。因此,必须通过过冷避免该范围。在粉红色蜡中添加0,25%-0,50%的硬脂酸可显着改善其硬度性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号