Comparative evaluation of marginal accuracy of metal copings fabricated using direct metal laser sintering, computer-aided milling, ringless casting, and traditional casting techniques: An In vitro study

机译:使用直接金属激光烧结,计算机辅助铣削,无环铸造和传统铸造技术制造的金属顶盖边缘精度的比较评估:一项体外研究

获取原文
           

摘要

Purpose: The purpose of the study is to determine the amount of marginal discrepancy produced by Co-Cr copings fabricated using various fabrication methods which include direct metal laser sintering (DMLS), computer-aided milling, traditional casting, and ringless casting and compare the values obtained between each fabrication technique and to evaluate if the fabrication technique can produce prosthesis that is within the standards of clinical acceptance of marginal discrepancy. Materials and Methods: Ten metal copings were fabricated by DMLS, computer-aided milling, traditional casting, and ringless casting. Marginal gap at the buccal, lingual, mesial, and distal areas was measured using silicone replica technique. A digital microscope was used to measure the silicone layer. Statistical analysis was done using one-way ANOVA test and post hoc Bonferroni test to test the difference between the fabrication method and categories of measured points, respectively. Results: The values indicate that the marginal gap was least for the copings fabricated using ringless casting followed by traditional casting and DMLS. The widest gap was seen in copings fabricated using computer-aided milling. Analysis of results showed statistically significant difference between copings fabricated using computer-aided milling and traditional casting (P = 0.029 and 0.043 – mesial and distal, respectively) and computer-aided milling and ringless casting (P = 0.002 and 0.001 – mesial and distal, respectively). Conclusion: Even though the marginal gap was found to vary with the fabrication method, all measurements of marginal gap of all groups were well within the standard clinical acceptance of 120 μ.
机译:目的:该研究的目的是确定使用各种制造方法(包括直接金属激光烧结(DMLS),计算机辅助铣削,传统铸造和无环铸造)制造的Co-Cr顶盖产生的边际差异量,并比较在每种制造技术之间获得的数值,并评估制造技术是否可以生产出在边缘差异临床接受标准内的假体。材料和方法:通过DMLS,计算机辅助铣削,传统铸造和无环铸造制造十种金属顶盖。使用硅胶仿制技术测量颊,舌,内侧和远端区域的边缘间隙。使用数字显微镜测量有机硅层。使用单向方差分析和事后Bonferroni检验进行统计分析,以分别检验制造方法和测量点类别之间的差异。结果:这些值表明,使用无环铸件,传统铸件和DMLS制成的顶盖的边缘间隙最小。在使用计算机辅助铣削加工的顶盖中发现了最大的间隙。结果分析显示,使用计算机辅助铣削和传统铸造制造的顶盖(分别为P = 0.029和0.043 –内侧和远端)与采用计算机辅助铣削和无环铸造制造的顶盖(P = 0.002和0.001 –中间和远端,分别)。结论:尽管发现边缘间隙随制造方法而变化,但所有组的边缘间隙的所有测量值均在120μs的标准临床接受范围内。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号