Research on testing method of resin sand high temperature compressive strength

机译:树脂砂高温抗压强度测试方法研究

获取原文
           

摘要

High temperature compressive strength is one of the most important performances of resin sand; its value directly concerns the quality of castings. In order to seek the best testing method of resin sand high temperature compressive strength, a self-developed instrument was used to carry out experiments, and the sample shape and size were designed and studied. The results show that a hollow cylinder sample can reflect the strength difference of different resin sands better than a solid cylinder sample, and its data is stable. The experiments selected フ20/5】30 mm as the size of the hollow cylinder samples. The high temperature compressive strengths of phenol-formaldehyde resin coated sand, furan resin self-setting sand, and TEA resin sand were each tested. For the resin sand used for cast steel and cast iron, 1,000 ìC was selected as the test temperature; for the resin sand used for cast non-ferrous alloy, 800 ìC was selected as the test temperature; and for all the resin sand samples, 1 min was selected as the holding time. This testing method can truthfully reflect the high temperature performance of three kinds of resin sand; it is reproducible, and the variation coefficients of test values are under 10%.
机译:高温抗压强度是树脂砂最重要的性能之一。它的价值直接关系到铸件的质量。为了寻求最佳的树脂砂高温抗压强度测试方法,采用自行研制的仪器进行实验,设计并研究了样品的形状和大小。结果表明,空心圆柱体样品比固态圆柱体样品能更好地反映不同树脂砂的强度差,其数据稳定。实验选择了φ20/ 5】30mm作为中空圆柱样品的尺寸。分别测试了酚醛树脂涂层砂,呋喃树脂自固化砂和TEA树脂砂的高温抗压强度。对于用于铸钢和铸铁的树脂砂,选择1000℃作为测试温度。对于用于铸造有色合金的树脂砂,选择800℃作为测试温度;对于所有树脂砂样品,选择1分钟作为保持时间。该测试方法可以真实地反映出三种树脂砂的高温性能。它具有可重现性,并且测试值的变异系数低于10%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号