The solidified structure of the thin-walled and complicated Ti-6Al-4V castings produced by the vertical centrifugal casting process was studied in the present work. The results show that the wall thickness of the section is featured with homogeneously distributed fine equiaxial grains, compared with the microstructure of the thick-walled section. The grain size of the castings has a tendency to decrease gradually with the increasing of the centrifugal radius. The inter-lamellar space in thick-walled casting parts is bigger than that of the thin-walled parts, and the profile of inter-lamellar space is not susceptible to the centrifugal radius.
机译:本文研究了通过垂直离心铸造工艺生产的薄壁且复杂的Ti-6Al-4V铸件的凝固组织。结果表明,与厚壁型材的显微组织相比,该型材的壁厚具有均匀分布的细等轴晶粒。铸件的晶粒尺寸具有随离心半径的增加而逐渐减小的趋势。厚壁铸件的层间空间比薄壁件大,层间空间的轮廓不受离心半径的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号