Optimization preparation of activated carbon from Enteromorpha prolifra using response surface methodology and its adsorption studies of fluoroquinolone antibiotics

机译:响应面法优化变形肠activated活性炭的制备及其对氟喹诺酮类抗生素的吸附研究。

获取原文
获取原文并翻译 | 示例
           

摘要

Enteromorpha prolifera, a marine solid waste abundantly available in Asia, was used as a low-cost precursor to prepare activated carbon (EPAC) using pyrophosphoric acid, H4P2O7, as a chemical activating agent. The effects of impregnation ratio, activation temperature and activation time on the specific surface area of the activated carbon were investigated through response surface methodology. The optimum preparation conditions were described as follows: impregnation ratio, 1.26; activation temperature, 455 degrees C; activation time, 48min. The characteristics of EPAC were examined by nitrogen adsorption-desorption isotherms, Fourier transformed infrared spectroscopy and scanning electron microscopy. The total pore volume and specific surface area of EPAC under optimum conditions were identified as 1.365cm(3)/g and 1124.1m(2)/g. The EPAC possessed high BJH pore volume, 1.276cm(3)/g and methylene blue value, 330mg/g, indicating the existence of abundant mesopores. The adsorption kinetic data of ciprofloxacin were well fitted to pseudo-second-order model, displaying a monolayer adsorption capacity for CIP of 216.55mg/g. The equilibrium data can be well described by Langmuir model. The dominant sorption mechanism is electrostatic attraction.
机译:Enteromorpha prolifera是一种在亚洲大量可用的海洋固体废物,被用作低成本前体,以焦磷酸H4P2O7作为化学活化剂来制备活性炭(EPAC)。通过响应面法研究了浸渍率,活化温度和活化时间对活性炭比表面积的影响。最佳的制备条件如下:浸渍比1.26;活化温度455℃;激活时间48分钟。通过氮气吸附-解吸等温线,傅立叶变换红外光谱和扫描电子显微镜检查了EPAC的特性。在最佳条件下,EPAC的总孔体积和比表面积被确定为1.365cm(3)/ g和1124.1m(2)/ g。 EPAC具有较高的BJH孔体积,为1.276cm(3)/ g,亚甲基蓝值为330mg / g,表明存在大量的中孔。环丙沙星的吸附动力学数据很好地拟合了伪二级模型,对CIP的单层吸附能力为216.55mg / g。平衡数据可以用Langmuir模型很好地描述。主要的吸附机制是静电吸引。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号