Effect of conditioning time of self-etching primers on dentin bond strength of three adhesive resin cements

机译:自酸蚀底漆的调理时间对三种胶粘剂树脂牙本质粘结强度的影响

获取原文
获取原文并翻译 | 示例
       

摘要

Objectives: To evaluate the effect of increasing the dentin conditioning time with self-etching primers of different aggressiveness (pH) on the microtensile bond strength (μTBS) of three resin cements. Materials and methods: Pre-cured composite blocks were cemented with M-Bond, Bistite II DC, or Panavia F to flat occlusal dentin surfaces of human third molars, which were conditioned with M-Bond or Bistite II-primer for 30, 60 or 180 s or with Panavia-primer for 60 or 180 s. Each dentin-composite block assembly (four in each group) was longitudinally sectioned to obtain 1 x 1 mm microbars and tested for the μJBS. The morphology of the conditioned dentin surface and the hybrid layer was examined with SEM. Results: Extending the primer conditioning time for Bistite II DC from 30 to 60 s significantly increased the μJBS (p < 0.001), but did not further increase from 60 s to 180 s. For M-Bond there was only a significant increase from 30 to 180 s(p < 0.05). For Panavia F the primer-conditioning time had no influence on the μTBS. SEM observations of conditioned dentin showed that the Bistite II DC and M-Bond self-etching primers with the lowest pH completely dissolved the dentin smear layer and plugs and formed well-defined hybrid layers. This was not found for Panavia F. Significance: Dentin bond strength of resin cements using more aggressive self-etching primers is improved by increasing the conditioning time. To enable resin infiltration of highly filled resin cements, sufficient smear layer dissolution is necessary.
机译:目的:评估使用不同侵蚀性(pH)的自蚀底漆增加牙本质调节时间对三种树脂水泥的微拉伸粘结强度(μTBS)的影响。材料和方法:将预固化的复合砌块与M-Bond,Bistite II DC或Panavia F粘合到人第三磨牙的平坦牙合面牙本质表面,然后用M-Bond或Bistite II-底漆处理30、60或60min。 180 s或使用Panavia底漆60或180 s。纵向切割每个牙本质复合块组件(每组四个),以获得1 x 1 mm的微棒,并测试μJBS。用SEM检查条件化的牙本质表面和杂化层的形态。结果:将Bistite II DC的引物调节时间从30 s延长到60 s,可显着增加μJBS(p <0.001),但从60 s到180 s没有进一步增加。对于M-Bond,仅从30 s到180 s显着增加(p <0.05)。对于Panavia F,引物调节时间对μTBS没有影响。 SEM对条件化牙本质的观察表明,具有最低pH值的Bistite II DC和M-Bond自蚀刻底漆完全溶解了牙本质涂片层并堵塞并形成了明确的杂化层。对于Panavia F而言,这没有发现。意义:通过增加调节时间,可以使用更具侵蚀性的自蚀底漆改善树脂水泥的牙本质粘结强度。为了使树脂能够渗透到高度填充的树脂胶结物中,必须充分涂抹污迹层。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号