SEM evaluation of resin-carious dentin interfaces formed by two dentin adhesive systems

机译:两种牙本质粘合体系形成的树脂-龋齿牙本质界面的SEM评价

获取原文
获取原文并翻译 | 示例
       

摘要

Objectives.: We investigated the influence of dentin tubule direction and identifiable zone of carious dentin on the microstructure and the thickness of the hybrid-like layer (HL) formed by self-etch and etch-rinse adhesive systems. Methods. : An etch-rinse and a self-etching adhesive were bonded to dentin carious zones divided into groups with parallel or perpendicular orientation relative to the dentin tubules at the resin-carious dentin interface (N = 5/variable). Bonds were prepared to each of the four zones of carious dentin apparent after staining with Caries Detector: pink, light pink, transparent and apparently normal; six non-carious third molars were controls. The microstructure and thickness of the HL were determined by SEM and compared using three-way ANOVA and Tukey's multiple comparisons (p < 0.05). Results. : Etch-rinse controls gave thicker HLs than self-etching systems; orientation did not affect thickness for the self-etch system. Perpendicular orientations gave thicker HLs than parallel for the pink zone bonded with the etch-rinse system. For both adhesives, HL thickness in the pink zone was significantly greater than in light pink for the perpendicular group, but no significant differences were found among other variables. HL microstructure was more granular and rougher for the etch-rinse than for the self-etching system. Pores and cracks were obvious in the more demineralized zones. Resin tags were shorter and irregular in the transparent zone and often were completely absent in the outer demineralized zones (pink, light pink). Significance. : Microstructure of bonded interfaces varies markedly depending on adhesive system, tubule orientation and carious zone.
机译:目的:我们研究了牙本质小管方向和龋齿的可识别区域对通过自蚀刻和蚀刻漂洗的粘合剂系统形成的混合样层(HL)的微观结构和厚度的影响。方法。 :在树脂-龋齿牙本质界面处,将浸蚀和自蚀粘合剂粘结到牙本质龋齿区域,该区域被划分为相对于牙本质小管具有平行或垂直方向的组(N = 5 /可变)。用龋齿检测器染色后,在龋牙本质的四个区域中的每个区域都准备好粘结:粉红色,浅粉红色,透明和看起来正常。六个非龋齿的第三磨牙为对照。 HL的微观结构和厚度通过SEM确定,并使用三向ANOVA和Tukey多重比较进行比较(p <0.05)。结果。 :与自蚀刻系统相比,蚀刻漂洗控件产生的HL更浓;取向不会影响自蚀刻系统的厚度。对于与蚀刻-冲洗系统结合的粉红色区域,垂直方向的HLs比平行方向的HLs厚。对于两种粘合剂,垂直组的粉红色区域中的HL厚度均明显大于浅粉红色,但在其他变量之间未发现显着差异。与自蚀刻系统相比,蚀刻冲洗的HL微结构更为颗粒和粗糙。在更矿化的区域中,毛孔和裂缝是明显的。透明区域的树脂标签较短且不规则,而外部脱盐区域(粉红色,浅粉红色)通常完全不存在。意义。 :粘合界面的微观结构根据粘合剂体系,肾小管方向和龋齿区的不同而有明显差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号