Objectives. To evaluate and compare bond strengths of different primers and resin cements to silica-based and zirconia ceramics.rnMethods. Silica-based and zirconia ceramic specimens were ground flat with #600-grit SiC paper. The ceramic surfaces were airborne-particle abraded and then divided into 11 groups of seven each: untreated (control); and conditioned with one of the six primers in combination with a resin cement from the same manufacturer as follows: Bistite II/Tokuso Ceramic Primer, Linkmax/GC Ceramic Primer, RelyX ARC/RelyX Ceramic Primer, Panavia F 2.0/Clearfil Ceramic Primer, and Resicem/Shofu Porcelain Primer and Resicem/AZ Primer. Stainless steel rods were bonded to the ceramic surfaces using one of the five resin cements. After 24-h water storage, the tensile bond strengths were tested using a universal testing machine and failure modes were examined.rnResults. Conditioning with primers containing a silane coupling agent (all the primers except AZ Primer) significantly enhanced bond strengths of resin cements to silica-based ceramic. For zirconia ceramic, Resicem/AZ Primer exhibited significantly higher bond strength than the other groups except Panavia F 2.0/Clearfil Ceramic Primer. The predominant failure mode of the groups conditioned with primers containing a phosphonic acid monomer (AZ Primer) or a phosphate ester monomer (Clearnl Ceramic Primer and Tokuso Ceramic Primer) was cohesive failure in cements whereas that with the other primers was adhesive failure at the zirconia surfaces.rnSignificance. The use of primers containing a silane coupling agent improved resin bonding to silica-based ceramic. On the other hand, the use of primers containing a phosphonic acid monomer or a phosphate ester monomer improved resin bonding to zirconia ceramic.
机译:目标。评估和比较不同底漆和树脂胶粘剂与二氧化硅基和氧化锆陶瓷的粘结强度。用#600粒度的SiC纸将二氧化硅基和氧化锆陶瓷样品磨平。陶瓷表面被空气颗粒磨蚀,然后分成11组,每组7组:未处理(对照);未处理并使用以下六种底漆之一与同一制造商的树脂胶泥组合使用:Bistite II / Tokuso陶瓷底漆,Linkmax / GC陶瓷底漆,RelyX ARC / RelyX陶瓷底漆,Panavia F 2.0 / Clearfil陶瓷底漆,以及Resicem / Shofu瓷底漆和Resicem / AZ底漆。使用五种树脂胶粘剂之一将不锈钢棒粘结到陶瓷表面。储水24小时后,使用万能试验机测试拉伸粘结强度,并检查破坏模式。用含有硅烷偶联剂的底漆(除AZ Primer以外的所有底漆)进行调理,可显着提高树脂胶泥与二氧化硅基陶瓷的粘结强度。对于氧化锆陶瓷,Resicem / AZ底漆的粘合强度比除Panavia F 2.0 / Clearfil陶瓷底漆以外的其他基团高得多。用含有膦酸单体(AZ底漆)或磷酸酯单体(Clearnl陶瓷底漆和Tokuso陶瓷底漆)的底漆处理的基团的主要破坏模式是水泥的内聚破坏,而其他底漆的氧化锆的粘结破坏是表面。意义。含有硅烷偶联剂的底漆的使用改善了树脂与二氧化硅基陶瓷的键合。另一方面,含有膦酸单体或磷酸酯单体的底漆的使用改善了树脂与氧化锆陶瓷的结合。

著录项

  • 来源
    《Dental materials》 |2010年第5期|p.426-432|共7页
  • 作者单位

    Cariology and Operative Dentistry, Department of Restorative Science, Graduate School, Tokyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-ku, Tofeyo 113-8549, Japan Global Center of Excellence (GCOE) Program, International Research Center for Molecular Science in Tooth and Bone Diseases at Tofeyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-feu, Tofeyo 113-8549, Japan;

    rnCariology and Operative Dentistry, Department of Restorative Science, Graduate School, Tokyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-ku, Tofeyo 113-8549, Japan;

    rnCariology and Operative Dentistry, Department of Restorative Science, Graduate School, Tokyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-ku, Tofeyo 113-8549, Japan;

    rnCariology and Operative Dentistry, Department of Restorative Science, Graduate School, Tokyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-ku, Tofeyo 113-8549, Japan;

    rnFaculty of Dentistry, School for Dental Technology, Tofeyo Medical and Dental University, 1-5-45 Yushima, Bunteyo-feu, Tofeyo 113-8549, Japan;

    rnDepartment of Conservative Dentistry, Floor 25, King's College London Dental Institute at Guy's, King's and St. Thomas' Hospitals, King's College London, London Bridge, London SE1-9RT, UK;

    rnGlobal Center of Excellence (GCOE) Program, International Research Center for Molecular Science in Tooth and Bone Diseases at Tofeyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-feu, Tofeyo 113-8549, Japan;

    rnCariology and Operative Dentistry, Department of Restorative Science, Graduate School, Tokyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-ku, Tofeyo 113-8549, Japan Global Center of Excellence (GCOE) Program, International Research Center for Molecular Science in Tooth and Bone Diseases at Tofeyo Medical and Dental University, 1-5-45 Yushima, Bunkyo-feu, Tofeyo 113-8549, Japan;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《化学文摘》(CA);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    zirconia ceramic; silica-based ceramic; resin cement; primer; acidic monomer; silane coupling agent; tensile bond strength; failure mode;

    机译:氧化锆陶瓷二氧化硅基陶瓷;树脂水泥底漆酸性单体硅烷偶联剂;抗拉强度故障模式;
  • 入库时间 2022-08-18 03:47:25

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号