Objective: The objective of this study is to evaluate the effect of a cleaning agent and priming on the bond strength (BS) of a resin cement (RC) to zirconia ceramics after 24 h and 1 year of water-storage. Materials and Methods: Fifty-six Katana and 56 ZirCAD zirconia ceramic plates were prepared and each zirconia brand was divided into four groups (n = 14): (1) untreated; (2) treated with Ivoclean cleaning agent; (3) treated with Monobond Plus coupling agent; (4) treated with Ivoclean + Monobond Plus. Cleaning and coupling agents were applied to zirconia following the manufacturers' instructions. The RC was manipulated, inserted into tubes (0.75 mm diameter/1 mm height) that were positioned on the zirconia surfaces and light activated. Specimens were tested after 24 h and 1 year of water storage. A shear load was applied to the base of the RC cylinders (until failure. Data were analyzed by three-way ANOVA and Tukey tests (α = 5%). Results: No significant difference in BS was noted between zirconia ceramics, except when the combination of cleaning and coupling agents was used. This combination increased the BS for Katana zirconia. One year of water storage leads to a decrease in BS for all experimental groups. Conclusion: The combination of cleaning agent and priming can yield higher BS for Katana at 24 h. BS to zirconia ceramics reduced approximately 50% after 1 year.
机译:目的:本研究的目的是评估清洁剂和底漆在储水24小时和1年后对树脂水泥(RC)与氧化锆陶瓷的粘结强度(BS)的影响。材料和方法:制备56种Katana和56种ZirCAD氧化锆陶瓷板,并将每个氧化锆品牌分为四组(n = 14):(1)未经处理; (2)用Ivoclean清洁剂处理; (3)用Monobond Plus偶联剂处理; (4)用Ivoclean + Monobond Plus处理。按照制造商的说明,将清洁剂和偶联剂应用于氧化锆。操纵RC,将其插入置于氧化锆表面上并被光激活的管子(直径0.75毫米/ 1毫米高)中。储水24小时和1年后对样品进行测试。将剪切载荷施加到RC圆柱体的底部(直到失效。通过三向ANOVA和Tukey测试(α= 5%)分析数据。结果:氧化锆陶瓷之间的BS值没有显着差异,除非当结论:清洗剂和底漆的组合可以使Katana氧化锆的BS更高。结合使用清洁剂和偶联剂可以提高Katana氧化锆的BS。 24 h。一年后,氧化锆陶瓷的BS降低了约50%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号