Determination of the sensitized zone extension in welded AISI 304 stainless steel using non-destructive electrochemical techniques

机译:使用无损电化学技术确定AISI 304焊接不锈钢的敏化区延伸

获取原文
获取原文并翻译 | 示例
           

摘要

Extension of sensitized zone (SZ) in welded AISI 304 stainless steel was determined by two non-destructive electrochemical tests: double loop electrochemical potentiokinetic reactivation technique (DLEPR) and local electrochemical impedance spectroscopy (LEIS). Welding was carried out using the shielded metal arc with two selected welding energies: the first one (0.7 kJ mm~(-1)) does not promote the sensitiza-tion of the 304 steel and it constitutes the reference sample and the second one (2.2kJmm~(-1)) which leads to the precipitation of chromium carbides in the grain boundaries after the welding process. The non-destructive DLEPR and LEIS tests allowed the length of the SZ to be determined and a good agreement between the two techniques and the microstructure of the two welded samples was shown. The presence of an inductive loop on the local impedance diagrams seems to reflect a galvanic coupling between the weld string (anode) and the welded stainless steel plates (cathode) which will be very prejudicial to a good corrosion resistance of the welded system. The results showed that the two electrochemical tests could be applied in practical cases in industrial field.
机译:焊接AISI 304不锈钢中的敏化区(SZ)的延伸通过两个无损电化学测试确定:双环电化学电位动力学再活化技术(DLEPR)和局部电化学阻抗谱(LEIS)。使用具有两种选定焊接能量的屏蔽金属电弧进行焊接:第一个(0.7 kJ mm〜(-1))不会促进304钢的敏化作用,它构成了参考样品,第二个( 2.2kJmm〜(-1))导致焊接后碳化铬在晶界析出。无损DLEPR和LEIS测试可以确定SZ的长度,并且两种技术之间的一致性很好,并且显示了两个焊接样品的微观结构。局部阻抗图上感应线圈的出现似乎反映了焊柱(阳极)与不锈钢焊接板(阴极)之间的电流耦合,这将对焊接系统的良好耐腐蚀性非常不利。结果表明,两种电化学测试方法均可在工业领域的实际应用中应用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号