首页> 外文期刊>Corrosion science >Corrosion of Al-Sn-Bi alloys in alcohol at high temperatures. Part I: Effects of the metallurgical structure of the alloys and the metal salt additions to alcohol
【24h】

Corrosion of Al-Sn-Bi alloys in alcohol at high temperatures. Part I: Effects of the metallurgical structure of the alloys and the metal salt additions to alcohol

机译:Al-Sn-Bi合金在高温下在醇中的腐蚀。第一部分:合金的冶金结构和向醇中添加金属盐的影响

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Corrosion of free machining Al alloys that contain Sn and Bi was investigated at 391-415 K in 2-(2-(2-methoxyethoxy)ethoxy)ethanol (MEEE) and 2-(2-(2-butoxyethoxy)ethoxy)ethanol (BEEE) with/without SnCl_2, Sn(OC_2H_5)_4, FeCl_3, and CuCl_2. The Al-Sn-Bi alloy displayed severe pitting corrosion in MEEE similar to the Al-Sn alloy in BEEE at 415 K, and Sn and Sn/Bi were enriched on the surface of pits. Immersion tests of pure Al in MEEE containing Sn/Cu-salts at 415 K also showed severe corrosion and the deposition of metallic Sn and Cu on the surface. The corrosion mechanisms are discussed in terms of the electro-catalytic activity of the Sn enriched on the surface.
机译:在391-415 K下研究了含Sn和Bi的自由加工铝合金在2-(2-(2-(2-甲氧基乙氧基)乙氧基)乙醇(MEEE)和2-(2-(2-丁氧基乙氧基)乙氧基)乙醇(含/不含SnCl_2,Sn(OC_2H_5)_4,FeCl_3和CuCl_2的BEEE)。 Al-Sn-Bi合金在MEEE中表现出严重的点蚀,与415 K时的BEEE中的Al-Sn合金相似,并且Sn和Sn / Bi富集在点蚀表面上。纯铝在415 K的含Sn / Cu盐的MEEE中的浸入测试还显示出严重的腐蚀以及金属Sn和Cu沉积在表面上。根据表面富集的Sn的电催化活性讨论了腐蚀机理。

著录项

  • 来源
    《Corrosion science》 |2010年第4期|1482-1491|共10页
  • 作者单位

    Graduate School of Engineering, Hokkaido University, N13-W8, Kita-Ku, Sapporo 060-8628, Japan;

    Graduate School of Engineering, Hokkaido University, N13-W8, Kita-Ku, Sapporo 060-8628, Japan;

    Graduate School of Engineering, Hokkaido University, N13-W8, Kita-Ku, Sapporo 060-8628, Japan;

    Graduate School of Engineering, Hokkaido University, N13-W8, Kita-Ku, Sapporo 060-8628, Japan;

    Center for Advanced Research of Energy Conversion Materials, Hokkaido University, N13-W8, Kita-Ku, Sapporo 060-8628, Japan;

    Asahikawa National College of Technology, Syunkohdai, 2-2, 1-6, Asahikawa 071-8142, Japan;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    A. Aluminum alloy; B. EPMA; C. Hot corrosion;

    机译:A.铝合金;B.EPMA;C.热腐蚀;