Properties Of Blended Cements With Thermally Activated Kaolin

机译:热活化高岭土掺合水泥的性能

获取原文
获取原文并翻译 | 示例

摘要

Kaolin, one of the materials of major importance for the ceramic and paper industry, is also used in the construction industry as a raw material for the production of white cement clinker and, in the form of metakaolin, as an artificial pozzolanic additive for concrete. Metakaolin is a vital component of high-performance and architectural concrete; however, its application in regular concrete is very limited due to relatively high production costs. This report evaluates the performance of a low-cost metakaolin-based additive called thermally activated kaolin (TAK), in cement. Due to its pozzolanic properties and the densification of cement matrix, the application of TAK provides a 15% improvement of the compressive strength. It was shown that TAK of optimal quality can be manufactured by the thermal treatment of raw kaolin with 74% of kaolinite at 750℃ without the intermediate beneticiation stage. The application of a developed approach can significantly reduce production expenditures and make the application of such an additive feasible even in regular-grade cement and concrete. kaolin; metakaolin; additive: thermal activation; cement; compressive strength; microslrueture
机译:高岭土是陶瓷和造纸工业中最重要的材料之一,在建筑业中还用作生产白水泥熟料的原料,并以偏高岭土的形式用作混凝土的人造火山灰添加剂。偏高岭土是高性能和建筑混凝土的重要组成部分。然而,由于相对较高的生产成本,其在常规混凝土中的应用非常有限。本报告评估了一种低成本的偏高岭土基添加剂,称为热活化高岭土(TAK)在水泥中的性能。由于其火山灰性质和水泥基质的致密化,TAK的应用可将抗压强度提高15%。结果表明,在74%的高岭土中,在750℃下对未经加工的高岭土进行热处理,可以制得质量最优的TAK。采用已开发的方法可以显着减少生产支出,并且即使在普通级水泥和混凝土中,也可以使用这种添加剂。高岭土偏高岭土;添加剂:热活化;水泥;抗压强度;微结构

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号