首页> 外文期刊>Construction and Building Materials >Durability of the adhesion between bituminous coatings and self-protection mineral granules of waterproofing membranes
【24h】

Durability of the adhesion between bituminous coatings and self-protection mineral granules of waterproofing membranes

机译:沥青涂料与防水膜自保护矿物颗粒之间粘附的耐久性

获取原文
获取原文并翻译 | 示例
           

摘要

Flat roofs in current buildings include a waterproofing system, often made of bituminous membranes with a self-protection constituted by mineral granules. These granules constitute the barrier against the fundamental environmental agent of degradation, the UV radiation. Therefore it is of paramount importance to understand the long-term performance of the self-protection layer, namely its adhesion to the coatings of bituminous membranes. This paper presents an experimental study on the behaviour of the self-protection granule of bituminous membranes when subjected to environmental agents of degradation. Different types of atactic polypropylene (APP) and styrene-butadiene-styrene (SBS) modified bituminous membranes, comprising different finishing systems, were exposed to the effects of elevated temperature and water for up to 24 weeks and 4 weeks, respectively. Following accelerated ageing, specimens of the different types of membranes were subjected to brushing tests, carried out according to EN 12039, in order to evaluate the adhesion of the self-protection granules. The results obtained in this study, which are compared with performance limits recommended by UEAtc directives, show that the higher loss of self-protection granule of bituminous membranes occurs in membranes modified by APP polymers. In addition, it was concluded that the effect of water is much more severe than that of elevated temperature.
机译:当前建筑物中的平屋顶包括防水系统,通常由沥青膜制成,并具有由矿物质颗粒构成的自我保护作用。这些颗粒构成了抵抗降解的基本环境因素,即紫外线辐射的屏障。因此,最重要的是了解自保护层的长期性能,即其对沥青膜涂层的附着力。本文对沥青膜的自我保护颗粒在环境降解剂作用下的行为进行了实验研究。包含不同涂饰系统的不同类型的无规聚丙烯(APP)和苯乙烯-丁二烯-苯乙烯(SBS)改性沥青膜分别暴露于高温和水的作用下,分别长达24周和4周。在加速老化之后,根据EN 12039对不同类型膜的样品进行刷涂测试,以评估自保护颗粒的附着力。这项研究获得的结果与UEAtc指令推荐的性能极限进行了比较,结果表明,沥青质膜自保护颗粒的损失较高,发生在APP聚合物改性的膜上。此外,得出的结论是,水的影响比升高的温度严重得多。

著录项

  • 来源
    《Construction and Building Materials》 |2011年第1期|p.138-144|共7页
  • 作者单位

    Department of Civil Engineering and Architecture, Institute Superior Tecnico/ICIST, Technical University of Lisbon. Av. Rovisco Pais 1, 1049-001 Lisboa, Portugal;

    National Laboratory of Civil Engineering (LNEC). Av. do Brasil 107. 1700-066 Lisboa, Portugal;

    Department of Civil Engineering and Architecture, Institute Superior Tecnico/ICIST, Technical University of Lisbon. Av. Rovisco Pais 1, 1049-001 Lisboa, Portugal;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    waterproofing; membrane; self-protection; granule; adhesion; durability;

    机译:防水膜;自我保护;颗粒;附着力耐用性;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号