Mechanical and hydration characteristics of autoclaved aerated concrete (AAC) containing iron-tailings: Effect of content and fineness

机译:含铁尾的高压灭菌加气混凝土(AAC)的机械和水合特性:含量和细度的影响

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

With the objective of reducing the negative impacts on environment and utilizing the secondary resource of tailings, the possibility of preparing AAC by using iron tailing was investigated. The bulk density and compressive strength were determined to indicating the feasibility of preparing AAC blocks from iron tailing. The morphology (FESEM-EDX), mineral constituent (XRD), thermal characteristics (TG-DSC) and crystal characteristics (29Si-NMR) of hydration products of AAC samples were analyzed to demonstrate the hydration characteristics of AAC products containing iron tailings effected by iron tailing content and fineness. The results indicated that the increasing content of iron tailing has negative effect on the mechanical property of AAC, and the finer of iron tailings can effectively enhance strength of AAC blocks. The main minerals in AAC products are C-S-H gel, tobermorite, anhydrite, hydrogarnet, and some residual minerals including quartz and calcite accompanied by ferric oxide and white mica in minor quantities. The increasing content of iron tailing obviously reduces the amount of calcium silicate hydrates; meanwhile, the finer of iron tailing accelerated the decomposition of white mica during the autoclaving process and has slight negative effect on crystallinity of tobermorite. It was also suggested that Al and Mg ions in iron tailings got into the structure of tobermorite during the hydrothermal reaction. This study provided the theoretical foundation for the utilizing of iron tailings in AAC production. (C) 2016 Elsevier Ltd. All rights reserved.
机译:为了减少对环境的不利影响并利用尾矿的二次资源,研究了使用铁尾矿制备AAC的可能性。测定堆积密度和抗压强度以表明由铁尾矿制备AAC块的可行性。分析了AAC样品水合产物的形态(FESEM-EDX),矿物成分(XRD),热特性(TG-DSC)和晶体特性(29Si-NMR),以证明受铁尾矿影响的AAC产物的水合特性铁尾矿含量和细度。结果表明,铁尾矿含量的增加对AAC的力学性能有不利影响,细的铁尾矿可以有效提高AAC砌块的强度。 AAC产品中的主要矿物质为C-S-H凝胶,雪铁矿,硬石膏,水榴石和一些残留矿物质,包括石英和方解石,以及少量的三氧化二铁和白云母。铁尾矿含量的增加明显减少了硅酸钙水合物的含量。同时,铁尾矿的细化加速了白云母在高压灭菌过程中的分解,并对雪铁矿的结晶度产生了轻微的负面影响。还表明在水热反应过程中,铁尾矿中的铝和镁离子进入了硅铁矿的结构。该研究为在AAC生产中利用铁尾矿提供了理论基础。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

  • 来源
    《Construction and Building Materials》 |2016年第15期|361-372|共12页
  • 作者单位

    Wuhan Univ Technol, State Key Lab Silicate Mat Architectures, Wuhan 430070, Peoples R China;

    Wuhan Univ Technol, State Key Lab Silicate Mat Architectures, Wuhan 430070, Peoples R China;

    Wuhan Univ Technol, State Key Lab Silicate Mat Architectures, Wuhan 430070, Peoples R China;

    Univ Ghent, Dept Struct Engn, Magnel Lab Concrete Res, Technol Pk Zwijinaarde 904, B-9052 Ghent, Belgium;

    Wuhan Univ Technol, State Key Lab Silicate Mat Architectures, Wuhan 430070, Peoples R China;

    Wuhan Univ Technol, State Key Lab Silicate Mat Architectures, Wuhan 430070, Peoples R China;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Autoclaved aerated concrete; Iron tailing; Content; Fineness; Mechanical property; Hydrothermal synthesis products;

    机译:蒸压加气混凝土;铁尾矿;含量;细度;机械性能;水热合成产品;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号