The Na2SO4-activated high-volume fly ash (Ns-activated HVFA) is a promising alternative to ordinary portland cement (OPC) due to its ecological and technical benefits. In this work, the effects of alkali dosage and silica fume incorporation on the flowability, setting time, compressive strength, porosity, composition and phase assemblage, and sulfate and acid resistance of Ns-activated HVFA are studied. The results show that an intermediate alkali dose at 2.5% by binder mass largely accelerates and enhances the strength development of HVFA. The synergic effect of Ns and silica fume further improves the strength of HVFA by about 20%. Exposure to the sodium sulfate solution can potentially promote the later activation of HVFA; while being exposed to the sulfuric acid solution, HVFA exhibits better resistance and less strength loss than the OPC-counterparts. The incorporation of silica fume negatively affects the acid resistance of Ns-activated HVFA. (C) 2021 Elsevier Ltd. All rights reserved.
机译:由于其生态和技术效益,Na2SO4活化的大容量粉煤灰(NS-Activated HVFA)是普通波特兰水泥(OPC)的有希望的替代品。在这项工作中,研究了碱剂量和二氧化硅烟雾的影响,研究了NS-活化HVFA的流动性,设定时间,抗压强度,孔隙率,组合物和相组合,以及硫酸盐和耐酸性。结果表明,通过粘合剂质量为2.5%的中间体碱剂量大部分加速和增强HVFA的强度发展。 NS和二氧化硅烟气的协同作用进一步提高了HVFA的强度约20%。暴露于硫酸钠溶液可以促进后来的HVFA活化;在暴露于硫酸溶液的同时,HVFA表现出比OPC对应物更好的抵抗和更少的强度损失。二氧化硅烟污的掺入负面影响NS-活化的HVFA的耐酸性。 (c)2021 elestvier有限公司保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号