The three-point bending tests were performed on the granite-mortar hybrid beam specimens to investigate the fracture properties of the interfacial transition zone (ITZ). Their curves of load versus crack mouth opening displacement were obtained. The peak load ratio and the fracture energy ratio between the hybrid specimen and the mortar specimen with the same water-cement ratio in mortar were introduced to characterize the weak ITZ fracture properties. The effects of the water-cement ratio in mortar, interface roughness and silica fume content in interfacial agent on the peak load and fracture energy were investigated and their relations were also fitted approximately. The results showed that both the peak load and fracture energy can be significantly increased by reducing the water-cement ratio in mortar and by increasing the granite-mortar interface roughness. However, the silica fume content has complicated nonlinear effects on the peak load and fracture energy. The optimal silica fume content is about 6%, which makes the best bonding performance between granite and mortar. (C) 2020 Elsevier Ltd. All rights reserved.
机译:在花岗岩砂浆混合束样本上进行三点弯曲试验,以研究界面过渡区(ITZ)的断裂性质。它们的负载曲线与裂缝口开口位移获得。引入了杂交试样与砂浆中相同水水柱比的脉搏试样与砂浆之间的峰值负荷率和裂缝能量比表征弱ITZ骨折性能。研究了砂浆,界面粗糙度和二氧化硅烟雾含量在斜率和骨折能量上的水水粘比的影响,并大致拟合了它们的关系。结果表明,通过降低砂浆中的水水粘器和增加花岗岩砂浆界面粗糙度,可以显着提高峰值负荷和断裂能量。然而,二氧化硅烟雾含量对峰值负荷和裂缝能量具有复杂的非线性效应。最佳的二氧化硅烟气含量约为6%,这使得花岗岩和砂浆之间的最佳粘合性能。 (c)2020 elestvier有限公司保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号