Effect of polypropylene plastic fibers length on cracking resistance of high performance concrete at early age

机译:聚丙烯塑料纤维长度对高性能混凝土早期抗裂性能的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Fibers reinforcement which is an effective mean to improve the cracking resistance of high performance concrete (HPC) is widely applied in practice. The early-age cracking resistance is improved by the addition of polypropylene plastic fibers, which is also affected by the length of fibers. Although investigations on the effect of content of polypropylene plastic fibers on the properties of HPC were carried out, investigations on the effect of length of polypropylene plastic fibers on the cracking resistance of HPC remain lacking. In present study, the effect of length of polypropylene plastic fibers on the early-age properties of HPC was investigated by Temperature Stress Test Machine. The test results and corresponding analysis indicated that: (1) the increasing length of polypropylene plastic fibers reduced the temperature drop at cracking time of HPC; (2) the increasing length of polypropylene plastic fibers reduced the absolute value of autogenous shrinkage of HPC; (3) the increasing length of polypropylene plastic fibers reduced the ratio of cracking stress to axial tensile strength and stress reserve of HPC; (4) the increasing length of polypropylene plastic fibers reduced the specific tensile creep of HPC; (5) the increasing length of polypropylene plastic fibers reduced the cracking resistance of HPC. (C) 2019 Elsevier Ltd. All rights reserved.
机译:纤维增强是提高高性能混凝土(HPC)抗裂性的有效手段,在实践中得到了广泛应用。聚丙烯塑料纤维的添加提高了早期抗龟裂性,而聚丙烯塑料纤维也受到纤维长度的影响。尽管已经进行了关于聚丙烯塑料纤维的含量对HPC性能的影响的研究,但是仍然缺乏关于聚丙烯塑料纤维的长度对HPC的抗裂性的影响的研究。在本研究中,通过温度应力试验机研究了聚丙烯塑料纤维的长度对HPC早期性能的影响。试验结果和相应的分析表明:(1)聚丙烯塑料纤维长度的增加减少了HPC裂解时间的温度下降; (2)聚丙烯塑料纤维长度的增加降低了HPC自发收缩的绝对值; (3)聚丙烯塑料纤维长度的增加降低了HPC的开裂应力与轴向拉伸强度之比和应力储备; (4)聚丙烯塑料纤维长度的增加降低了HPC的比拉伸蠕变; (5)聚丙烯塑料纤维长度的增加降低了HPC的抗裂性。 (C)2019 Elsevier Ltd.保留所有权利。

著录项

  • 来源
    《Construction and Building Materials》 |2020年第may30期|117874.1-117874.10|共10页
  • 作者

  • 作者单位

    Hohai Univ Coll Civil & Transportat Engn 1 Xikang Rd Nanjing 210098 Peoples R China|Jiangsu Engn Res Ctr Crack Control Concrete 1 Xikang Rd Nanjing 210098 Peoples R China|Nanjing Engn Res Ctr Prefabricated Construct 1 Xikang Rd Nanjing 210098 Peoples R China;

    Jiangsu Engn Res Ctr Crack Control Concrete 1 Xikang Rd Nanjing 210098 Peoples R China|Nanjing Engn Res Ctr Prefabricated Construct 1 Xikang Rd Nanjing 210098 Peoples R China|Nanjing Construct Grp CO Ltd 200 Ruanjian Ave Nanjing 210012 Peoples R China;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    High performance concrete; Polypropylene plastic fibers; Early age; Tensile creep; Cracking resistance;

    机译:高性能混凝土;聚丙烯塑料纤维;早年;拉伸蠕变抗裂性;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号