Application of a capillary crystalline material to enhance cement grout for sealing tunnel leakage

机译:毛细晶状材料在水泥灌浆中的应用,用于密封隧道渗漏

获取原文
获取原文并翻译 | 示例
           

摘要

This study investigates the feasibility of using a cement-based capillary crystalline material, Penetron Admix (PA), to enhance the performance of a cement grout for sealing tunnel leakage. A series of experiments were carried out to investigate the effects of PA on the viscosity, setting time, concretion rate, permeability and compressive strength of the cement grout. The experimental results show that inclusion of PA into cement grout has no effect on its viscosity and setting time, but can markedly increase the concretion rate, and the compressive strength of the grout concrete and reduce its permeability. Micro structure characterizations by CT scanning indicate that cement-gravel grout concrete samples with additional PA show a compact and smooth structure compared to those without PA; SEM images show that the dendritic crystals are observable under high magnification in the cement grout concrete samples with PA, and the number of crystals increases as the amount of PA increases. Based on the experimental results and the micro structure characterizations, it can be concluded that PA can be used as an additive to improve the rate of concretion, compressive strength, and impermeability of cement grout. To achieve an optimum leakage-sealing effect, the weight ratio of PA to cement of 1.4-1.6% is recommended. (C) 2019 Elsevier Ltd. All rights reserved.
机译:这项研究调查了使用水泥基毛细管结晶材料Penetron Admix(PA)来增强水泥灌浆密封隧道渗漏的性能的可行性。进行了一系列实验,研究了PA对水泥浆的粘度,凝结时间,凝结速率,渗透性和抗压强度的影响。实验结果表明,将PA掺入水泥浆中不会对其粘度和凝结时间产生影响,但可显着提高水泥混凝土的固结速率和抗压强度,并降低其渗透性。通过CT扫描的微观结构表征表明,与不含PA的水泥-砾石浆混凝土样品相比,不含PA的水泥-砾石浆混凝土样品具有致密而光滑的结构; SEM图像显示,在具有PA的水泥灌浆混凝土样品中,在高放大倍率下可观察到树枝状晶体,并且随着PA含量的增加,晶体数量增加。根据实验结果和微观结构特征,可以得出结论,PA可以用作提高水泥浆凝结率,抗压强度和抗渗性的添加剂。为了获得最佳的密封效果,建议PA与水泥的重量比为1.4-1.6%。 (C)2019 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号