A study of the replacement of desulphurization slag for sand to ready-mixed soil materials (RMSM)

机译:将砂中的脱硫渣替代为预拌土壤材料(RMSM)的研究

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

After the industrial of steelmaking by-products are processed properly, they can be used in civil engineering, not only as a substitute for natural resources and to reduce costs, but also to provide environmental protection. This study used different amounts (10%, 20%, 30%, 40%, and 50%) of desulphurization slag to replace natural fine aggregates in ready-mixed soil materials, and tested the physical and fresh properties (slump, slump flow, tube flow, initial setting time, and bleeding) and hardened properties (compressive strength, ball drop, ultrasonic pulse velocity) of the materials. The variations between the performances of the materials with different mix proportions were discussed. When desulphurization slag is used in RMSM, the workability can be enhanced obviously significantly. When the replacement of desulphurization slag is 50%, the slump flow is increased by 110mm compared with the control group, and the initial setting time increases as the replacement increases, because of bleeding. When the replacement is 10% and 20%, the compressive strength at various ages is higher than that of the control group. When the replacement is 10%, the compressive strength at 7 days is higher than that of the control group by 60%, and the ultrasonic pulse velocity is proportional to the compressive strength, which increases with age and decrease as the replacement increases. An appropriate replacement can effectively accelerate construction, and allow projects to be finished ahead of schedule; therefore, an appropriate replacement, is applicable for ready-mixed soil materials.
机译:炼钢副产品工业得到适当加工后,它们可用于土木工程,不仅可以替代自然资源并降低成本,而且还可以提供环境保护。这项研究使用了不同数量(分别为10%,20%,30%,40%和50%)的脱硫矿渣替代了预拌土壤材料中的天然细骨料,并测试了其物理和新鲜特性(坍落度,坍落度,管的流动,初始凝固时间和渗出)以及材料的硬化性能(抗压强度,落球,超声脉冲速度)。讨论了不同混合比例的材料性能之间的差异。在RMSM中使用脱硫渣可明显提高可加工性。当脱硫渣的替代量为50%时,坍落流量与对照组相比增加了110mm,并且初始替代凝结时间会随着出血量的增加而增加。当替换为10%和20%时,各个年龄段的抗压强度均高于对照组。当替代量为10%时,第7天的抗压强度比对照组高60%,超声脉冲速度与抗压强度成正比,随着年龄的增长而增加,随着替代量的增加而降低。适当的更换可以有效地加快建设速度,并允许项目提前完成;因此,适当的替代品适用于预拌的土壤材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号