The influence of the laminate thickness, stacking sequence and thermal aging on the static and dynamic behavior of carbon/epoxy composites

机译:层压板厚度,堆叠顺序和热老化对碳/环氧树脂复合材料静态和动态行为的影响

获取原文
获取原文并翻译 | 示例
           

摘要

In this work, we investigate the influence of laminate thickness, stacking sequence and thermal aging on the damping behavior of carbon/epoxy laminates. The dynamic behavior of quasi-isotropic and unidirectional laminates of different thickness, are measured by means of Laser Doppler Vibrometry and Dynamic Mechanical Analysis. Obtained results before and after aging at 175 ℃ for 250 and 500 h, are compared with static strength properties. The Laser Doppler Vibrometry measurements of the modal damping factors, show general increasing tendency for the unidirectional composites after aging, but decreasing tendency for quasi-isotropic plates. The DMA damping measurements reveal an increase of the damping in longitudinal direction after aging, but a decrease in transverse direction. Comparison of results of dynamic measurements with static properties, confirm that mechanism of damping in composite structures depends mainly on stacking sequence. Moreover, modal damping of unidirectional composites depends mainly on the properties of the fiber-matrix interface, while damping of the quasi-isotropic laminates is affected by long-term properties of the matrix. Thus, to ensure long term damping performance of the carbon/epoxy components subjected to vibrations, one should take into account the stability of the matrix and fiber-matrix interfaces and also the alignment of the reinforcing fibers.
机译:在这项工作中,我们研究了层压板厚度,堆叠顺序和热老化对碳/环氧层压板阻尼行为的影响。通过激光多普勒振动法和动态力学分析来测量不同厚度的准各向同性和单向层合物的动力学行为。将在175℃老化250和500 h之前和之后获得的结果与静态强度性能进行比较。模态阻尼因子的激光多普勒振动测量表明,单向复合材料在老化后总体上呈上升趋势,而准各向同性板则呈下降趋势。 DMA阻尼测量显示,老化后纵向阻尼增加,而横向阻尼减少。将动态测量结果与静态特性进行比较,确认复合结构的阻尼机制主要取决于堆叠顺序。此外,单向复合材料的模态阻尼主要取决于纤维-基体界面的特性,而准各向同性层合物的阻尼则受基体的长期特性影响。因此,为了确保经受振动的碳/环氧组分的长期阻尼性能,应考虑基质和纤维-基质界面的稳定性以及增强纤维的排列。

著录项

  • 来源
    《Composite Structures》 |2014年第12期|208-216|共9页
  • 作者单位

    AGH University of Science and Technology, al. Mickiewicza 30, 30-059 Krakow, Poland,Delphi Technical Center Krakow, ul. Podgorki Tynieckie 2, 30-399 Krakow, Poland;

    AGH University of Science and Technology, al. Mickiewicza 30, 30-059 Krakow, Poland;

    AGH University of Science and Technology, al. Mickiewicza 30, 30-059 Krakow, Poland;

    AGH University of Science and Technology, al. Mickiewicza 30, 30-059 Krakow, Poland;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Polymer-matrix composites; Environmental degradation; Durability; Vibration; Damping factors; Thermal aging;

    机译:聚合物基复合材料;环境恶化;耐用性振动;阻尼系数;热老化;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号