With respect to the minimization of fatigue cracking in flexible pavements, it is widely recognized that current SUPERPAVE specification criteria do not allow a reliable ranking of the fatigue resistance of bituminous binders. Thus, an alternative characterization procedure, based on the use of time sweep testing protocols and on the concept of Dissipated Energy Ratio (DER), has been proposed within NCHRP Project 9-10. However, the true significance of test results still needs to be thoroughly understood in order to define new acceptance and grading criteria.rnIn this paper the Authors present the results obtained during an experimental investigation which addressed the issue of fatigue damage of modified binders and mastics. In particular, the objective of the study was to highlight, by means of time sweep tests, the effects on the fatigue behaviour caused by variations of the type and dosage of the polymer used as a chemical modifier. Moreover, the same kind of test was carried out on bituminous mastics in order to gain a better understanding of the role played by mineral filler in the fatigue performance of the binding matrix.rnIn the analysis of test results, for a more complete description of the damage behaviour of the materials during cyclic loading, a new parameter, based on dissipated energy data, was introduced. Such a parameter, called Relative Crack Propagation Amplitude (RCPA), proved to be especially useful in highlighting the peculiar effects caused by the creation within the binder mass of an effective fatigue-resistant polymer network, in differentiating the consequences deriving from the use of different polymer types and dosages, and in comparing the performance of mastics with that of the corresponding binders.
机译:关于最小化柔性路面中的疲劳裂纹,众所周知,当前的SUPERPAVE规范标准不能可靠地对沥青粘合剂的抗疲劳性进行排名。因此,已经在NCHRP项目9-10中提出了基于时间扫描测试协议和耗散能量比(DER)概念的替代表征程序。然而,为了定义新的验收和分级标准,仍然需要彻底理解测试结果的真正意义。在本文中,作者介绍了在实验研究中获得的结果,该研究解决了改性粘合剂和胶泥的疲劳损伤问题。特别地,该研究的目的是通过时间扫描测试来突出由用作化学改性剂的聚合物的类型和剂量的变化对疲劳行为的影响。此外,对沥青胶泥进行了相同类型的测试,以便更好地了解矿物填料在粘结基体疲劳性能中的作用。在测试结果分析中,对沥青的更完整描述循环加载过程中材料的损伤行为,基于耗散能量数据,引入了一个新参数。事实证明,这种参数称为“相对裂纹扩展幅度”(RCPA)在突出由有效的抗疲劳聚合物网络在粘合剂团块中形成所引起的特殊效果,区分因使用不同而产生的后果方面特别有用。聚合物类型和剂量,以及乳胶与相应粘合剂的性能比较。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号