Comparison of the Oxidation of Phenol with Iron and Copper Supported on Activated Carbon from Coconut Shells

机译:椰壳活性炭负载铁和铜负载的铁和铜氧化苯酚的比较。

获取原文
获取原文并翻译 | 示例
       

摘要

Home-made Fe/activated carbon (Fe/AC) and Cu/activated carbon (Cu/AC) catalysts were tested for the wet oxidation of phenol in a standard wet oxidation unit (Trickle Bed Reactor), at the bench scale and under strong conditions (453-473 K and P = 30 atm). A complete conversion of phenol was reached at 473 K and 30 atm with the Fe/AC catalyst at a metal load of 2 %, while maximum conversion with the Cu/AC catalyst was 75 % with a metal load of 2 %. The Fe/AC catalyst was also found to have good chemical stability under changes of temperature and pH. The results show that the oxidation of phenol takes place on the catalyst surface via a heterogeneous mechanism, whilst the contribution of the homogeneous reaction was not significant. Some oxidation intermediates were identified, consisting of ring intermediates (p-benzoquinone, p-hydroxybenzoic acid and traces of hydroquinone), which were further oxidized to short chain acids (mainly maleic, malonic, acetic and formic acids).
机译:在标准湿法氧化装置(滴流床反应器)中,在台式规模和强力条件下,测试了自制的Fe /活性炭(Fe / AC)和Cu /活性炭(Cu / AC)催化剂的苯酚湿氧化。条件(453-473 K,P = 30 atm)。 Fe / AC催化剂在2%的金属负载下,在473 K和30 atm时苯酚完全转化,而Cu / AC催化剂在2%的金属负载下最大转化率为75%。还发现Fe / AC催化剂在温度和pH变化下具有良好的化学稳定性。结果表明,苯酚的氧化是通过非均相机理在催化剂表面发生的,而均相反应的贡献并不显着。鉴定出一些氧化中间体,由环中间体(对苯醌,对羟基苯甲酸和痕量对苯二酚)组成,它们被进一步氧化成短链酸(主要是马来酸,丙二酸,乙酸和甲酸)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号