Glazed ceramics -both original and replacement- from Chamberf Metro Station (built in 1919) in Madrid (Spain) were studied using a multidisciplinary approach aimed at finding out more about the materials and technologies used to make them. The original white tiles, which help illuminate these underground spaces, were manufactured in Onda, Castellon (Spain) with very calcareous clays fired at approximate to 950 degrees C and coated with lead alkali-glazes. The original decorative pieces, with a metallic sheen, were made in Triana, Seville (Spain) with calcareous and illite clays fired at temperatures of between 850 and 950 degrees C and treated with transparent lead glazes. The replacement pieces had the same appearance as the originals but were more resistant. The white tiles were made out of quartz-rich, illite-kaolinite and calcareous clays fired at temperatures of 950 degrees C with an alkali-glazes that was very rich in zircon and aluminium. The decorative pieces were made from illite-kaolinite clays very rich in aluminium and fired at 850 degrees C. These included an additive in the form of a highly refractory grog and were covered with an aluminium-rich lead-potassium glaze. The manufacturing techniques used to make each type of piece varied depending on their particular function within the station.
机译:玻璃陶瓷 - 从Madrid(西班牙)的Chouderf地铁站(1919年建于1919年)的玻璃陶瓷,采用多学科方法研究了旨在更多地了解用于制造它们的材料和技术。有助于照亮这些地下空间的原始白色瓷砖在ONDA,Castellon(西班牙)中制造,具有非常钙质粘土,近似为950℃并涂有铅碱釉料。使用金属光泽的原始装饰件是在Triana,塞维利亚(西班牙)中制造的,钙质和岩石粘土在850至950℃的温度下烧制,并用透明的引线釉处理。替换件具有与原件相同的外观,但更具抗性。白色瓷砖由石英,伊利石岩石和钙质粘土制成,在> 950℃的温度下用锆和铝的碱性釉料烧制。装饰件由富含铝的illite-koolinite粘土制成,并在<850℃下烧制。这些包括高度耐火格粒形式的添加剂,并用富含富含富含铝的铅玻璃釉料覆盖。用于使每种类型的制造技术根据其特定功能而变化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号