Hydrophilic, flexible polyurethane (FPU) foams made from Hypol prepolymers are capable of retaining large amounts of water and saline solutions. The addition of different catalysts and surfactant agents to Hypol JM 5008 prepolymer was assayed to obtain a foam with good structural stability and elasticity. The combination of three catalysts, stannous octoate and two amine-based ones (Tegoamin 33 and Tegoamin BDE), and the surfactant Niax silicone L-620LV allowed to synthesize a foam with a homogeneous cell size distribution, exhibiting the highest saline absorption capacity (2.4 g/gram of foam) and almost complete shape recovery, with up to a 20% of remaining deformation. Then, superabsorbent sodium acrylate polymer (PNaA) was added to the FPU foam up to 8 pph. The urine absorption capacity of the foam was increased about 24.8% by incorporating 6 pph of PNaA, absorbing 17.46 g of saline solution per foam gram, without any negative impact on the rest of the foam properties. All these properties make the synthesized foams suitable for corporal fluids absorption applications in which elasticity and low-density are required.
机译:由腹水预聚物制成的亲水性,柔性聚氨酯(FPU)泡沫能够保持大量的水和盐溶液。在测定中添加不同催化剂和表面活性剂试剂以获得泡沫,以获得具有良好结构稳定性和弹性的泡沫。三种催化剂,辛酸辛酸盐和两种基于胺基(Tegoamin 33和Tegoamin BDE)的组合,以及表面活性剂NIAX硅氧烷L-620LV允许用均匀的细胞尺寸分布合成泡沫,表现出最高的盐水吸收能力(2.4 g /克泡沫)和几乎完全的形状恢复,剩余变形的高达20%。然后,将超吸收性丙烯酸钠聚合物(PNAA)加入到最高可达8pph的FPU泡沫中。通过在PNAA的6pph掺入6pph,泡沫的尿液吸收能力增加约24.8%,每泡克吸收17.46g盐水溶液,对泡沫特性的其余部分没有任何负面影响。所有这些属性使合成的泡沫适用于只需要弹性和低密度的体内流体吸收应用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号