This study proposes different manufacturing techniques (manual pelletization, powder pressing, and “shell scaffold”) to obtain lightweight clay ceramics containing recovery raw materials. The sintering in an electrical furnace (1000 °C, 1 h processing time) was conducted by traditional firing from room temperature, for pressed and shell-scaffold samples, while the flash heating (i.e., samples directly put at 1000 °C) was used only for the pellets. The porous materials (porosity 40–80%), functionalized with nutrients (K and P) in amounts to confer the fertilizer capability, gave suitable results in terms of pH (6.7–8.15) and electrical conductivity (0.29–1.33 mS/cm). Thus, such materials can be considered as feasible lightweight clay ceramics, with a positive effect on the soil. These findings permit us to hypothesize a potential use in green roofs or in agronomic applications.
机译:本研究提出了不同的制造技术(手动造粒,粉末压制和“壳支架”),以获得含有回收原料的轻质粘土陶瓷。电炉(1000℃,1h处理时间)中的烧结是通过室温的传统烧制进行的,用于压制和壳支架样品,而闪蒸加热(即直接放置1000°C的样品)只针对颗粒。用营养素(K和P)赋予肥料能力的多孔材料(孔隙率40-80%),以pH(6.7-8.15)和电导率(0.29-1.33ms / cm)提供合适的结果。因此,这种材料可以被认为是可行的轻质粘土陶瓷,对土壤产生积极影响。这些调查结果允许我们假设绿色屋顶或农艺应用中的潜在用途。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
代理获取

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号